This study investigates the utilization of Ti/Ni reactive multilayer foils as an energy source for facilitating the joining of Ni–Ti shape memory alloys through diffusion bonding. Multilayered samples were prepared using a 10-cycle accumulative roll bonding (ARB) process to be used for the bonding process. Diffusion bonding employing reactive multilayers was conducted over a temperature range of 600 °C to 900 °C, at 5 MPa pressure, with a 1-h hold time. Additionally, a comparison was made with a diffusion-bonded Nitinol sample at 900 °C without a reactive multilayer. Materials characterization and testing involved scanning electron microscopy (SEM), energy-dispersive spectroscopy (EDS), shear strength testing, and differential scanning calorimetry (DSC), which were conducted on the bonded samples. The findings underscored the advantages of using reactive multilayers for diffusion bonding. These benefits included the formation of TiNi and the induction of a shape memory effect in the joint region, alongside a 1.5 times shear strength compared to identical diffusion bonding conditions without reactive multilayers. Moreover, employing reactive multilayers in the diffusion bonding of Nitinol holds promise for significantly reducing the energy needed to achieve robust and seamless bonded boundaries in the joining area.
3 April 2024 in Advances in Materials and Processing Technologies
Theorists, experimentalists, and industrialists have all acknowledged that further improvements of electrical steel (ES) magnetic properties using the current chemical composition (< 3.2wt% Si) and conventional manufacturing routes remain extremely challenging. However, to enable the prevailing vehicle and aircraft electrifications revolution, further developments in materials and electrical machine designs are required. Today, additive manufacturing (AM) unlocks opportunities to produce steels with high Si content (> 6.5wt% Si) which are otherwise unprocessed through conventional thermomechanical route due to the brittle nature of high-silicon alloys. However, challenges around their inferior magnetic properties remain to be overcome. Here, a novel in situ coating, i.e., lamination during 3D printing of 6.5% Si steel is demonstrated. The in situ steel lamination via “Successive Building and Coating” approach was conducted through a combination of powder coating and printing strategies that enabled a production of a near net shape laminated high Si electrical steel. The Ar atomized 6.5% Si steel powder was coated with (Mn, Zn) ferrite via sol–gel auto-combustion method and with SiO 2 via sol–gel method for comparison purposes. The coated powder was fused in the ProX300 Laser Powder Bed Fusion to build successive and insulated layer-by-layer structure of high Si steel parts. The in situ lamination was successfully achieved; however, the coating layers were non-uniform and occasionally discontinuous. It was concluded that the distance between the coating layers varies and cannot be correlated to powder thickness layer. It is demonstrated that a higher powder layer thickness ( L ) results in a thicker and non-uniform insulating coat layer during in situ lamination; therefore, a smaller L was recommended. Furthermore, the successive layer-by-layer formation of a matrix coat perpendicular to building direction indicated that Buoyancy effect was affected by other factors that directly influenced the metallic–ceramic melt pool dynamics. Finally, it is demonstrated that ferrimagnetic (Mn 0.8 ,Zn 0.2 )Fe 2 O 4 -laminated samples possess superior magnetic properties compared to amorphous SiO 2 -laminated samples.