Aim. The purpose of this study is to investigate the effects of hydrofluoric acid and one‐component ceramic primer and silane (Monobond Etch and Prime (MEP)) applications on lithium disilicate glass ceramics and zirconium‐infiltrated lithium silicate glass ceramics, as well as the effect of ultrasonic and phosphoric acid surface washing methods on bond strength. Materials and Method. A total of 240 ceramic samples were prepared using two different CAD‐CAM material blocks with a thickness of 2 mm made of lithium disilicate glass‐ceramic (IPS e.max CAD) and zirconium‐infiltrated lithium silicate glass ceramic blocks (Celtra Duo). The samples were cemented to the composite discs (Tetric N‐Ceram) after two different acid treatments, and surface washing processes were applied to them. As such, 24 groups were formed, each with two different acid applications, three different washing processes, two different CAD‐CAM blocks, and two different aging procedures (n = 10). Following the application of the acid, different washing processes are used. These were HF acid and washing only (HF + W), HF acid and ultrasonic washing (HF + US), HF acid and phosphoric acid (HF + PA), MEP with washing only (MEP + W), MEP and ultrasonic washing (MEP + US), and MEP and phosphoric acid (MEP + PA). The composite discs were cemented with dual cure adhesive cement (Multilink Automix) after the determined surface treatments were applied to the blocks. After surface applications, SEM analysis was conducted. Following exposure to two different thermal procedures, long‐term (TL) and short‐term (TS), bond strengths were measured using an Instron universal test device. SPSS version 23.0 software was used to perform the statistical analyses. Histogram graphs and the Kolmogorov‐Smirnov/Shapiro‐Wilk test were used to assess the variables’ conformity to the normal distribution. Results. The bond strength values of TS and TL in the Celtra Duo block were significantly higher than those in the e.max CAD block (p < 0.05). The TS‐TL bonding strength value difference in the e.max CAD block was significantly higher than the surface measurements in the Celtra Duo block. While the highest bond strength value HF + US for TS in e.max CAD was 20.07 ± .31, the values of HF + US in Celtra Duo were significantly higher in terms of TL values when compared to other groups. Conclusion. Celtra Duo material demonstrated higher bond strength values after a short and long thermal cycle than e.max CAD material. In general, groups bonded with HF were less affected by the thermal cycle than groups treated with MEP.
27 March 2023 in Journal of Health Sciences and Medicine
Aim: New treatment options have been developed as alternative post-retaining restorations and crowns that preserve remaining tooth tissue in endodontically treated teeth with excessive substance loss. This study, current treatment approaches newly graduated, intern and doctoral or specialist dentists in teeth excessive coronal destruction were evaluated. Material and Method: This cross-sectional study, online questionnaire consisting of 22 questions, 3 parts was applied. First part consists of demographic information participants, second part consists of questions measuring awareness about preferred indirect restorations, last part consists of current treatment approaches newly graduated, intern and doctoral or specialist dentists. Total 234 voluntary participants questionnaires were evaluated. Obtained data were analyzed with IBM SPSS V23. Results: In restoration of endodontically treated buccal mesial walls (least 2 mm thick) molars, participants all 3 groups preferred posterior adhesive indirect restorations according to their titles. Considering level of awareness, participants high group preferred posterior adhesive indirect restorations more in restorations endodontically treated buccal lingual walled molar teeth. Participants all 3 groups preferred use fiber under composite strengthen teeth in the restoration of teeth with excessive substance loss. Conclusion: According to the results, it was determined that awareness and knowledge level of dentists who received specialty or doctoral training about new current treatments was higher than other newly graduated and intern dentists. It was observed that participants group with high level awareness mostly preferred posterior region indirect adhesive restorations such as endocrown and onlay.
In computer-aided design/computer-aided manufacturing (CAD/CAM) restorations for severely damaged teeth, the cavity floor or proximal margins may be elevated with composite resin to improve adhesion. This in vitro study investigated how different surface pretreatment methods affect the shear bond strength (SBS) of hybrid CAD/CAM materials to dentin or composite surfaces, simulating clinical situations of composite elevation. Hybrid CAD/CAM samples were bonded to dentin or composite substrates following different surface pretreatment protocols and cemented using a dual-cure adhesive resin cement. The samples were thermocycled and subjected to shear bond strength testing, and failure modes were analyzed. The SBS in the sandblasting (SB)+Dentin group and hydrofluoric acid (HF)+Dentin was significantly higher than that in the SB+Composite and HF+Composite groups (p < 0.05). Untreated+composite and untreated+dentin groups showed significantly lower SBS (p < 0.05). Failure mode analysis revealed a predominance of cohesive failures in the SB+Dentin group, while adhesive failures were more frequently observed in most of the other groups. SB-treated and HF-etched hybrid CAD/CAM materials showed more favorable bonding behavior to dentin than to composite, highlighting that bonding to the elevated composite layer may be less effective than bonding directly to prepared dentin.