This experiment investigated the mechanical performance and acid resistance (when subjected to 28 days of exposure to sulfuric and nitric acid of five percent) of ambient-cured geopolymer concrete. Geopolymer concrete (GPC)—which is produced by using industrial by-products, including fly ash and ground granulated blast furnace slag (GGBS)—is a low-carbon and strong substitute of Ordinary Portland Cement (OPC). This experiment examines the mechanical and acid-resisting properties of ambient GPC with different GGBS (10, 30, and 50 percent) contents. The compressive, tensile, and flexural strengths were measured at 7, 14, and 28 days, and durability was measured under an exposure of 5% sulfuric and nitric acids. X-ray diffraction (XRD) and scanning electron microscopy (SEM) showed that gypsum and ettringite were formed by sulfuric acid that weakened the structure, whereas surface decalcification was mostly caused by nitric acid. Mixes with a high fly ash content had more amorphous structures and better acid resistance, whereas those having high GGBS contents had high early strength because of high densities of the C–A–S–H gel. The findings indicate a strength–durability trade-off, which can be used to control the optimized mix design to produce sustainable and long-term infrastructure.
There is a significant problem in Middle Eastern countries with respect to climate change and rainwater management. This research discusses the influence of water-cement ratio (W/C) and aggregate size on pervious concrete strength and permeability. In this research, the impact of different aggregate sizes with different water-cement ratios are examined in the pervious concrete. The main results are that pervious concrete with a 0.4 water-cement ratio and a coarse aggregate of 10 mm got the highest compressive strength (15.7 MPa at 7 days, 16.83 MPa at 28 days). The results show that the W/C directly influenced compression strength, whereas the coarse aggregate’s size directly affected water content, increasing strength. Pervious concrete made with 10 mm aggregate was found to have better compressive strength, flexural strength, and permeability than 20 mm aggregate. Due to working ability, paste coating, and paste density, it acquires strength with a slightly higher water-cement ratio. With a somewhat higher water-cement ratio, the paste contained fewer open pores, which improved the load transfer and enhanced the compressive strength. The void content in the pervious concrete was considerably higher than that of standard concrete, which influenced the formation and strength of hydration products. These findings are instrumental in tuning the performance of pervious concrete to different conditions, especially when its application needs to be more sustainable.