Three strategies were proposed to prolong the service life of continuous fiber-reinforced silicon carbide ceramic matrix composite (CMC-SiC), which served as thermal-structure components of aeroengine at thermo-mechanical-oxygenic coupling environment. As for some thermal-structure components with low working stress, improving the degree of densification was crucial to prolong the service life, and the related process approaches were recited. If the thermal-structure components worked under moderate stress, the matrix cracking stress (σmc) should be improved as far as possible. The fiber preform architecture, interface shear strength, residual thermal stress, and matrix strengthening were associated withσmcin this review. Introducing self-healing components was quite significant with the appearance of matrix microcracks when CMC-SiC worked at more severe environment for hundreds of hours. The damage can be sealed by glass phase originating from the reaction between self-healing components and oxygen. The effective self-healing temperature range of different self-healing components was first summarized and distinguished. The structure, composition, and preparation process of CMC-SiC should be systematically designed and optimized to achieve long duration target.
Porous Si3N4-Si3N4 composite ceramics were fabricated by 3D printing combined with low-pressure chemical vapor infiltration (CVI). This technique could effectively improve the designability of porous Si3N4 ceramics and optimize the mechanical and dielectric properties. The effects of process parameters including the deposition time and heat treatment on the microstructure and properties of porous Si3N4-Si3N4 composite ceramics were studied. The study highlights following: When CVI processing time was increased from 0 to 12 h, the porosity decreased from 68.65% to 26.07% and the density increased from 0.99 to 2.02 g/cm3. At the same time, the dielectric constant gradually increased from 1.72 to 3.60; however, the dielectric loss always remained less than 0.01, indicating the excellent electromagnetic (EM) wave-transparent performance of porous Si3N4-Si3N4 composite ceramics. The maximum flexural strength of 47±2 MPa was achieved when the deposition time attained 6 h. After heat treatment, the porosity increased from 26.07% to 36.02% and the dielectric constant got a slight increase from 3.60 to 3.70 with the dielectric loss still maintaining lower than 0.01. It has been demonstrated that the porous Si3N4-Si3N4 composite ceramics are a promising structural and EM wave-transparent material suitable for high temperature service.
20 July 2023 in Journal of the European Ceramic Society
The SiBCN matrix via chemical vapor infiltration (CVI) or/and polymer infiltration pyrolysis (PIP) technologies was orderly introduced to SiCf/SiC composites to optimize the mechanical property and electromagnetic (EM) shielding effectiveness simultaneously. The BN interface with the thickness of 350 nm was designed to obtain a little stronger interface bonding. The flexural strength of SiCf/SiC-SiBCN composites reached 545.45±29.59 MPa thanks to the crack deflection between the CVI SiC and CVI SiBCN, as well as CVI SiBCN and PIP SiBCN matrix because of the modulus difference between them. The fracture toughness (KIC) with the value of 16.02±0.94 MPa·m1/2 was obtained owing to the extension of crack propagation path. The adverse effect of stronger interface bonding was eliminated by the design of matrix microstructure for SiCf/SiC-SiBCN composites. The thermal conductivity in the thickness direction was 7.64 W·(m·K)−1 at 1200 °C and the electric resistivity decreased to 1.53×103 Ω·m. The tunable dielectric property was obtained with the coordination of wave-absorption CVI SiBCN matrix and impedance matching PIP SiBCN matrix, and the total shielding effectiveness (SET) attained 30.01 dB. It indicates that the SiCf/SiC-SiBCN composites have great potential to be applied as structural and functional materials.