Three strategies were proposed to prolong the service life of continuous fiber-reinforced silicon carbide ceramic matrix composite (CMC-SiC), which served as thermal-structure components of aeroengine at thermo-mechanical-oxygenic coupling environment. As for some thermal-structure components with low working stress, improving the degree of densification was crucial to prolong the service life, and the related process approaches were recited. If the thermal-structure components worked under moderate stress, the matrix cracking stress (σmc) should be improved as far as possible. The fiber preform architecture, interface shear strength, residual thermal stress, and matrix strengthening were associated withσmcin this review. Introducing self-healing components was quite significant with the appearance of matrix microcracks when CMC-SiC worked at more severe environment for hundreds of hours. The damage can be sealed by glass phase originating from the reaction between self-healing components and oxygen. The effective self-healing temperature range of different self-healing components was first summarized and distinguished. The structure, composition, and preparation process of CMC-SiC should be systematically designed and optimized to achieve long duration target.
We report on the growth of SiC nanowires on a single crystal Si substrate by pyrolysis of polycarbosilane and using two catalyst (Al2O3 and Ni) films with different thickness (2, 4, and 6 nm). The catalyst films were deposited on the Si substrate, and the SiC nanowires were grown according to two mechanisms, i.e., the oxide-assisted growth mechanism and vapor- liquid-solid mechanism. As a result, pearl-chain-like SiC nanowires and straight SiC nanowires were obtained. The prepared nanowires exhibited excellent photoluminescence properties, emission spectra displaying two emission peaks at 395 and 465 nm, and have good thermal stability below 1000 °C. The experimental results revealed the importance of the catalyst in controlling the morphology and properties of SiC nanowires.
The implementation of SiC fiber reinforced SiC/SiC composites to aero-engine hot components has attracted wide attention, due to their many excellent properties. Along these lines, in order to predict the oxidation behavior of the material in extreme environments and to explore the effect of different preforms on the oxidative behavior of the composites, four SiC/SiC composites, with different preforms, were oxidized under environmental conditions of pressure of 12 kPa H2O:8 kPa O2:80 kPa Ar, at 1400 °C temperature. Moreover, the morphology and defect distribution of the samples were characterized by carrying out scanning electron microscopy, and micro-computed X-ray tomography measurements. Furthermore, the relation between the micro- and macro-scales was established, so as to be able to predict the oxidation behavior of the composites; not only the quantitative relationship between the mass change rate and the defect volume change rate, but also the combination of micro-computed X-ray images.
High−performance bolts made of carbon/carbon (C/C) composites are necessary for connecting thermally−insulating structural components of aerospace vehicles. To enhance the mechanical properties of the C/C bolt, a new silicon infiltration−modified C/C (C/C−SiC) bolt was developed via vapor silicon infiltration. The effects of silicon infiltration on microstructure and mechanical properties were systematically studied. Findings reveal that dense and uniform SiC−Si coating has been formed after silicon infiltration of the C/C bolt, strongly bonding with the C matrix. Under tensile stress, the C/C−SiC bolt undergoes a tensile failure of studs, while the C/C bolt is subject to the pull−out failure of threads. The breaking strength of the former (55.16 MPa) is 26.83% higher than the failure strength of the latter (43.49 MPa). Under double−sided shear stress, both the crushing of threads and the shear failure of studs occur within two bolts. As a result, the shear strength of the former (54.73 MPa) exceeds that of the latter (43.88 MPa) by 24.73%. According to CT and SEM analysis, matrix fracture, fiber debonding, and fiber bridging are the main failure modes. Therefore, a mixed coating formed by silicon infiltration can effectively transfer loads from coating to carbon matrix and carbon fiber, thereby enhancing the load−bearing capacity of C/C bolts.