Antibacterial and pH-responsive composite films for active food packaging were fabricated based on polyvinyl alcohol (PVA), cassava starch, ethyl lauroyl arginate (LAE), and mulberry anthocyanin. With the incorporation of LAE and mulberry anthocyanin, the PVA/starch blend films exhibited a less compact and more heterogeneous surface structure. The tensile strength and elongation at break of the active films were not significantly affected when the mulberry anthocyanin content was less than 20%. Moreover, the incorporation of mulberry anthocyanin effectively improved the UV barrier property of the blend films. Notably, while mulberry anthocyanin showed obvious color changes in buffer solutions with different pH values, the changes were indistinguishable for the PVA/starch/mulberry anthocyanin films. By contrast, the color changes of the PVA/starch/LAE/mulberry anthocyanin films were more noticeable, indicating the addition of LAE increased the pH sensitivity of the blend films. Furthermore, the PVA/starch/LAE/mulberry anthocyanin films efficiently inhibited the growth of both Escherichia coli (E. coli) and Staphylococcus aureus (S. aureus) due to the strong antibacterial activity of LAE. According to the spoilage test, the active films containing 5% mulberry anthocyanin and 5% LAE effectively indicated and slowed down the spoilage process of dairy milk. Our results demonstrate that PVA/starch/LAE/mulberry anthocyanin films have high potential as bioactive packaging materials applied in the food industry.
Different characterization methods spanning length scales from molecular to micron scale were applied to inspect the microstructures and mechanical/hydrophilic features of agar/konjac glucomannan (KGM) films prepared under different drying temperatures (40 and 60 °C). Note that the lower preparation temperature (40 °C) could increase the strength and elongation of agar/KGM films at high KGM levels (18:82 wt/wt KGM-agar, or higher). This was related to the variations in the film multi-scale structures with the increment of KGM content: the reduced crystallinity, the increased perfection of nanoscale orders at some KGM amounts, and the negligibly-changed morphology and molecular chemical structure under 40 °C preparation temperature. These structural changes initially decreased the film tensile strength, and subsequently increased the film strength and elongation with increasing KGM content. Moreover, under the higher drying temperature (60 °C), the increased KGM content could concurrently reduce the strength and elongation for the films, associated with probable phase separations on nano and smaller scales. In addition, the increased KGM amount tended to make the film more hydrophilic, whereas the changes in the film structures did not dominantly affect the changing trend of hydrophilicity.
1 December 2021 in International Journal of Biological Macromolecules
A novel dextranase was purified from Penicillium cyclopium CICC-4022 by ammonium sulfate fractional precipitation and gel filtration chromatography. The effects of temperature, pH and some metal ions and chemicals on dextranase activity were investigated. Subsequently, the dextranase was used to produce dextran with specific molecular mass. Weight-average molecular mass (Mw) and the ratio of weight-average molecular mass/number-average molecular mass, or polydispersity index (Mw/Mn), of dextran were measured by multiple-angle laser light scattering (MALS) combined with gel permeation chromatography (GPC). The dextranase was purified to 16.09-fold concentration; the recovery rate was 29.17%; and the specific activity reached 350.29 U/mg. Mw of the dextranase was 66 kDa, which is similar to dextranase obtained from other Penicillium species reported previously. The highest activity was observed at 55 °C and a pH of 5.0. This dextranase was identified as an endodextranase, which specifically degraded the α-1,6 glucosidic bonds of dextran. According to metal ion dependency tests, Li+, Na+ and Fe2+ were observed to effectively improve the enzymatic activity. In particular, Li+ could improve the activity to 116.28%. Furthermore, the dextranase was efficient at degrading dextran and the degradation rate can be well controlled by the dextranase activity, substrate concentration and reaction time. Thus, our results demonstrate the high potential of this dextranase from Penicillium cyclopium CICC-4022 as an efficient enzyme to produce specific clinical dextrans.
A novel bio-adsorbent was fabricated via grafting an amino-terminated hyperbranched polymer (HBP-NH2) onto bagasse cellulose. The morphology and microstructure of the HBP-NH2-grafted bagasse cellulose (HBP-g-BC) were characterized and its adsorption capacity for Cr(VI) ions in aqueous solutions was investigated. The rough surface structure of HBP-g-BC that is beneficial for improving the adsorption capacity was observed by scanning electron microscopy (SEM). The grafting reaction was confirmed by Fourier-transform infrared (FT-IR) spectroscopy. The adsorbent performance was shown to be better with a lower pH value, a higher adsorbent dosage, or a higher initial Cr(VI) concentration. Moreover, the kinetics study revealed that the adsorption behavior followed a pseudo-second-order model. The isotherm results showed that the adsorption data could be well-fitted by the Langmuir, Freundlich, or Temkin models. Moreover, HBP-g-BC could maintain 74.4% of the initial removal rate even after five cycles of regeneration. Thus, the high potential of HBP-g-BC as a bio-adsorbent for heavy metal removal has been demonstrated.