22 December 2025 in Molecules
Verified
Journal Article
Open access
PDF file
Irina ZverevaIrina Zvereva
Irina Zvereva
ASAzamat Samadov
Azamat Samadov
SKSergei Alekseevich Kurnosenko
Sergei Alekseevich Kurnosenko
SKSergey Kirichenko
Sergey Kirichenko
MSMarina G. Shelyapina
Marina G. Shelyapina
VPVitalii Petranovskii
Vitalii Petranovskii
This study investigates the influence of mesoporosity, pre-created by alkali etching in ZSM-5 zeolite, on the characteristics of Fe3+ ion-exchange and subsequent changes in its textural and optical properties. It is shown that the formed hierarchical porosity facilitates the penetration of hydrated iron complexes into the internal channels. This not only increases the degree of exchange, but also leads to the formation of multinuclear FexOy clusters and, possibly, to the partial isomorphic replacement of Al3+ with Fe3+ in the framework. Comprehensive characterization of mesoporous samples (XRD, SEM, N2 adsorption, UV-Vis) confirms the preservation of the microporous crystal structure of MFI on the one hand, and demonstrates a significant change in the distribution of iron-containing species in mesoporous matrices on the other. The introduction of Fe ions significantly reduces the bandgap energy, shifting the absorption edge into the visible range. The results obtained demonstrate that preliminary mesostructuring is an effective approach for creating hierarchically porous Fe zeolites with great potential for photocatalytic applications.

25 December 2025 in Molecules
Verified
Journal Article
Open access
PDF file
Irina ZverevaIrina Zvereva
Irina Zvereva
Denis PankratovDenis Pankratov
Denis Pankratov
EZElena Zemstova
Elena Zemstova
VKVladimir Kudymov
Vladimir Kudymov
ASAzamat Samadov
Azamat Samadov
VPVitalii Petranovskii
Vitalii Petranovskii
Alkaline treatment in 0.2 and 0.4 M NaOH solutions successfully generated controlled mesoporosity into ZSM-5 (Zeolite Socony Mobil-5) zeolite, resulting in average mesopore diameters of approximately 15 and 25 nm, respectively, while preserving the crystalline structure of the zeolite framework. Parent ZSM-5 and its mesoporous derivatives obtained by desilication were used to prepare (Fe species)@(zeolite matrix) composites. The synthesis was carried out by co-precipitating Fe2+/Fe3+ ions onto both parent and desilicated ZSM-5 matrices under oxygen-free conditions. Comprehensive characterization by X-ray diffraction, scanning electron microscopy, N2 adsorption, vibrating-sample magnetometry, 57Fe Mössbauer spectroscopy, and diffuse reflectance UV–Vis spectroscopy revealed that the degree of introduced mesoporosity dramatically influences the size, dispersion, phase composition, and oxidation state of the iron-containing nanospecies. On purely microporous ZSM-5, relatively large (~15 nm) partially oxidized magnetite nanoparticles are formed predominantly on the external surface, exhibiting superparamagnetism at room temperature (Mₛ = 11 emu/g) and a band gap of 2.12 eV. Increasing mesoporosity leads to progressively smaller and more highly dispersed iron(III) oxo/hydroxo clusters with significantly lower blocking temperatures and reduced magnetization (down to 0.7 emu/g for Fe@ZSM-5_0.4). All composites display strong visible-light absorption confirming their potential as magnetically separable visible-light-driven photocatalysts for environmental remediation.

1 December 2024 in Russian Journal of Physical Chemistry A
Verified
Journal Article
Closed access
PDF file
Irina ZverevaIrina Zvereva
Irina Zvereva
MSMarina G. Shelyapina
Marina G. Shelyapina
IMI. A. Minich
I. A. Minich
YAY. A. Anufrikov
Y. A. Anufrikov
OSOleg Silyukov
Oleg Silyukov
VPVitalii Petranovskii
Vitalii Petranovskii
This work presents the results of the study of glycerol and water sorption using two complimentary approaches, simultaneous thermal analysis and isothermal sorption calorimetry, on zeolites differing in the framework topology and post modifications (natural clinoptilolite, protonated zeolite ZSM-5 with Si/Al ratio of 50, commercial Na-mordenite with Si/Al ratio of 6.5 then modified by ion exchange for copper ions, or by alkaline etching to develop mesoporosity, and pillared mordenite). For the studied mordenites a correlation between texture and composition and sorption capacity towards glycerol and water was shown. Analysis of glycerol and water desorption suggests the optimal temperature range for catalytic conversion of glycerol via dehydration and carboxylation.

29 October 2026 in Catalysts
Verified
Journal Article
Open access
PDF file
Irina ZverevaIrina Zvereva
Irina Zvereva
Farid OrudzhevFarid Orudzhev
Farid Orudzhev
ASAzamat Samadov
Azamat Samadov
SKSergei Alekseevich Kurnosenko
Sergei Alekseevich Kurnosenko
AMAsiyat Magomedova
Asiyat Magomedova
VPVitalii Petranovskii
Vitalii Petranovskii
Hierarchical porosity and iron speciation govern the balance between adsorption and catalytic oxidation in Fe-modified ZSM-5. This study compares a microporous low-iron material, Z0–Fe0.1 (0.9 wt.% Fe), with a hierarchically porous high-iron material, Z0.4–Fe1.0 (25 wt.% Fe). Structural, textural, optical, X-ray photoelectron, and Mössbauer characterization was combined with methylene blue removal experiments under adsorption, photocatalytic, Fenton-like, and photo-Fenton-like conditions. Both materials retained the MFI structure. UV–Vis analysis indicated a greater relative contribution of oligomeric FexOy species in Z0.4–Fe1.0. Mössbauer spectroscopy identified predominantly Fe3+ environments and revealed a magnetically ordered component in the high-iron material at 78 K. Despite an almost 28-fold difference in iron loading, both materials achieved nearly identical final methylene blue removal (~99%) under photo-Fenton-like conditions, yet this similar efficiency was reached through fundamentally different dominant pathways: predominantly adsorption for the microporous Z0–Fe0.1 (dark adsorption ~82%) and predominantly catalytic oxidation for the hierarchical Z0.4–Fe1.0 (dark adsorption only ~38%, rising to ~87% under dark Fenton-like conditions). These results indicate a shift in the balance between adsorption and H2O2-dependent removal accompanying changes in porosity and iron loading. The findings highlight the need to consider pore architecture, adsorption, and iron speciation jointly when interpreting the performance of Fe-containing zeolites for water treatment.