The article studies the influence of chlorosulfonated polyethylene CSM 40 as a compatibilizer on the curing characteristics of the rubber compound, dynamic mechanical analysis, morphology, physico-mechanical and performance properties of vulcanized rubber based on a compound of ethylene propylene diene monomer EPDM S 501A and nitrile butadiene NBR 2645 rubbers. DMA studies indicate that the temperature dependence of tanδ for vulcanizates with and without a compatibilizer based on EPDM S 501A/NBR 2645 at a ratio of 75/25 parts per hundred parts of rubber (phr) has a bimodal character, which indicates the incompatibility of the rubber phases. The temperature dependence for EPDM S 501A/NBR 2645 vulcanizates (25/75 phr) with and without a compatibilizer has a monomodal form, which characterizes the improved compatibility of the rubber phases. SEM showed that a clearly defined microporous structure is observed on a cleavage of vulcanizate sample EPDM/NBR (25/75 phr) without a compatibilizer; with the addition of CSM 40, this feature is retained, but becomes less pronounced. It is shown that vulcanizates containing the compatibilizer CSM 40 are characterized by increased strength properties and hardness compared to vulcanized rubber without a compatibilizer. It was established that the vulcanized rubber based on EPDM S 501A/NBR 2645/CSM 40 (25/75/5 phr) is characterized by the smallest changes in the elastic-strength properties and hardness of vulcanizates after a day of thermo-oxidative aging in air and their weight after exposure to industrial oil I-20A and standard petroleum fluid SZhR-1 at room temperature among vulcanizates based on EPDM S 501A and NBR 2645. The vulcanizate of the rubber compound, including a compound of EPDM/NBR (25/75 phr) with a compatibilizer CSM 40 in an amount of 5 phr (2.88 wt.%), is characterized by stable physico-mechanical properties and improved performance properties. This rubber compound can be used for the manufacture of rubber products operating under the influence of oils and hydrocarbon environments.
Crystalline lanthanide terephthalates, Ln2bdc3‧nH2O (Ln = La–Lu, excluding Pm), were synthesized using a surfactant-free, ultrasound-assisted method. This approach yielded microcrystals with diverse shapes and sizes ranging from 2 to 10 μm. Notably, under these conditions, lutetium terephthalate uniquely crystallized as Lu2(1,4-bdc)3·2.5H2O, while the remaining lanthanides formed tetrahydrate terephthalates, Ln2bdc3‧4H2O (Ln = La–Nd, Sm–Yb).
This paper discusses the processes of the long-lived 137Cs and 60Co immobilization on titanium surfaces in simulated light water reactor primary circuit environments. This study is prompted by numerous problems in both the maintenance of equipment during reactor operation and the dismantling of the reactor after the completion of the operation, which is associated with contamination of working surfaces with long-lived radionuclides. The composition of the oxide films formed on the surface of commercial titanium alloy ПT-3B has been studied with specimens prepared in autoclave test conditions and surface samples from the pipeline sections to which the primary coolant was applied. These films on the coolant pipeline surface consist of a titanium dioxide layer tightly adhered to the pipeline metal surface and weakly fixed deposits—crystallites comprised of titanium oxides and other corrosion products (oxides and hydrated oxides of iron, nickel, chromium etc.). The radionuclide composition of the samples was studied by gamma-spectrometry. It is shown that the mechanism of titanium-surface contamination with 137Cs is by physisorption, contamination level increases upon the presence of dispersed particles. For 60Co, both sorption and deposition onto surfaces are observed.