Al–Zn–Ca alloys are good candidates for industrial electronics and electric vehicles due to their high thermal conductivity, castability, and corrosion resistance, but their strength requires improvement. This study investigates how Sc and Zr additions affect the microstructure, thermal, mechanical, and corrosion properties of an Al–3 wt% Zn–3 wt% Ca base alloy. Microstructural analysis showed that substituting Sc with Zr did not drastically alter the phase composition but changed the elemental distribution: Sc was uniform, while Zr segregated to center of dendritic cell. Zr addition also refined the grain size from 488 to 338 μm. An optimal aging treatment at 300 °C for 3 h was established, which enhanced hardness for all alloys via precipitation of Al3Sc/Al3(Sc,Zr) particles. However, this Zr substitution reduced thermal conductivity (from 184.7 to 168.0 W/mK) and ultimate tensile strength (from 269 to 206 MPa), though it improved elongation at fracture (from 4.6 to 7.1%). All aged alloys exhibited high corrosion resistance in 5.7% NaCl + 0.3% H2O2 water solution, with Zr-containing variants showing a lower corrosion rate and better pitting resistance. The study confirms the potential of tuning Sc/Zr ratios in Al–Zn–Ca alloys to achieve a favorable balance of strength, ductility, thermal conductivity, and corrosion resistance.
Al–Zn–Ca alloys are good candidates for industrial electronics and electric vehicles due to their high thermal conductivity, castability, and corrosion resistance, but their strength requires improvement. This study investigates how Sc and Zr additions affect the microstructure, thermal, mechanical, and corrosion properties of an Al–3wt%Zn–3wt%Ca base alloy. Microstructural analysis showed that substituting Sc with Zr did not drastically alter the phase composition but changed the elemental distribution: Sc was uniform, while Zr segregated to dendritic cores. Zr addition also refined the grain size from 488 to 338 μm. An optimal aging treatment at 300 °C for 3 hours was established, which enhanced hardness for all alloys via precipitation of Al3Sc/Al3(Sc,Zr) particles. However, this Zr substitution reduced thermal conductivity (from 184.7 to 168.0 W/mK) and ultimate tensile strength (from 269 to 206 MPa), though it improved elongation at fracture (from 4.6 to 7.1%). All aged alloys exhibited high corrosion resistance in 5.7% NaCl + 0.3% H2O2 solution, with Zr-containing variants showing a lower corrosion rate and better pitting resistance. The study confirms the potential of tuning Sc/Zr ratios in Al–Zn–Ca alloys to achieve a favorable balance of strength, ductility, thermal conductivity, and corrosion resistance.
4 July 2026 in International Journal of Corrosion and Scale Inhibition
A two-stage technological process for the preparation of two-color decorative plasma electrolytic coatings on the AD31 aluminum alloy has been developed. At the first stage, plasma electrolytic treatment of the aluminum alloy should be carried out in a silicate electrolyte with addition of boric acid. At this stage, a coating with low through porosity is formed due to isomorphic substitution of silicon by boron in its oxide and, as a result, a decrease in its melting temperature. Evidence for the latter effect after the formation of the plasma electrolytic coating in a silicate–borate electrolyte includes: the formation of denser coating layers with a fused surface morphology; higher values of anodic and cathodic voltage amplitudes in plasma electrolytic treatment; the appearance of a small amount of crystalline phases in the coating based on amorphous silicon oxide; a decrease in the number of anodic plasma microdischarges per unit area of the treated aluminum alloy surface accompanied by an increase in the power released in these discharges; a decrease in anodic current density upon polarization of AD31 alloy samples with a plasma electrolytic coating. At the second stage, incorporation of a coloring component into the silicate–borate electrolyte ensures the formation of decorative two-color coatings upon plasma electrolytic treatment of the aluminum alloy.