Magnesium alloys are usually considered as structural materials when the weight reduction is important - in aircraft and space industry for example. In recent years, there has been an increase in the use of new generation ignition-proof high-strength magnesium alloys in the design of aircraft parts. The properties of new ignition-proof casting magnesium alloys ML-OPB (Mg–6.7Y–2.6Zn–0.5Zr–0.35Ce– 0.35Yb; wt.%) and EWZ43 (Mg–3.8Y–4.4Nd–0.6Zr–0.6Zn; wt.%) were investigated and compared with properties of commercial magnesium alloys. The microstructure of investigated alloys in the as-cast condition comprises of a magnesium solid solution and a significant amount of eutectic. Heat treatment according to the T6 mode results in change in the eutectic phase’s morphology and also to their partial dissolution in the magnesium matrix. Long-term high-temperature holding, simulating operating conditions (500 h at 300 °C), leads to the formation of precipitates along the grain boundaries in both alloys, significantly reducing the mechanical properties. During the oxidation of the samples, it was established that the main components that involved into the oxide film and provides the protective properties of the alloys is Y, Nd and Yb. The investigated alloys have a high strength, which is not lower than that of the ML10 alloy. At the same time, the advantage of the ML-OPB alloy is a high elongation at fracture, while the EWZ43 alloy is characterized by high strength. The corrosion rate of the investigated alloys exceeds the corrosion rate of known commercial ML10 and AZ91 alloys, which implies the need for additional protection against corrosion of investigated alloys. At the same time, the castability of ML-OPB and EWZ43 alloys is no lower than that of most commercial magnesium alloys. An oxide film with high Y content and high protective properties is formed when the alloys interact with the sand mold bonded with furan resin. The ignition temperature of the investigated alloys is 100–150 °C higher than that of the ML10 alloy. The flammability test of alloys in the flame of a gas burner, made on cone samples and typical aircraft castings «bracket», showed that ML-OPB and EWZ43 alloys are almost non-flammable under the conditions of experiment.
The phase composition of VZhL14N-VI nickel superalloy was analyzed in a wide temperature range – from room temperature to 1600 °C by means of CALPHAD (CALculation of PHAse Diagrams) calculations. In light of the findings, the authors devised potential heat treatment modes for VZhL14N-VI superalloy. The impact of different heat treatment modes on the grain size, hardness, and electrical conductivity of VZhL14N-VI superalloy samples produced by ceramic mold casting was investigated, as well as the effect on the alloy of high-temperature annealing at 1070 – 1170 ℃ for 1 – 4 h. The alloy heat treatment resulted in a notable increase in grain size and a decrease in hardness. The influence of artificial aging temperature after high-temperature annealing and quenching on the hardness and electrical conductivity of the alloy in the range of 610 – 810 ℃ was studied. At 810 °C, the alloy exhibits the most pronounced aging effect, accompanied by a rapid increase in hardness, reaching approximately 370 HV. In contrast to the observed changes in hardness, the electrical conductivity of the alloy exhibited minimal variation during the aging process. The proposed heat treatment conditions diverge from those recommended by the OST 1 90126–85 Russian standard for this alloy. The developed heat treatment mode includes the alloy heat treatment at a temperature of 1170 ± 10 ℃ for 4 h, followed by air cooling and aging at a temperature of 810 ± 10 ℃ for 10 – 14 h, followed by air cooling. The proposed heat treatment mode is expected to result in an increase in hardness of VZhL14N-VI superalloy castings by 10 – 20 HV in comparison to the samples subjected to the standard heat treatment mode.
Al–Zn–Ca alloys are good candidates for industrial electronics and electric vehicles due to their high thermal conductivity, castability, and corrosion resistance, but their strength requires improvement. This study investigates how Sc and Zr additions affect the microstructure, thermal, mechanical, and corrosion properties of an Al–3 wt% Zn–3 wt% Ca base alloy. Microstructural analysis showed that substituting Sc with Zr did not drastically alter the phase composition but changed the elemental distribution: Sc was uniform, while Zr segregated to center of dendritic cell. Zr addition also refined the grain size from 488 to 338 μm. An optimal aging treatment at 300 °C for 3 h was established, which enhanced hardness for all alloys via precipitation of Al3Sc/Al3(Sc,Zr) particles. However, this Zr substitution reduced thermal conductivity (from 184.7 to 168.0 W/mK) and ultimate tensile strength (from 269 to 206 MPa), though it improved elongation at fracture (from 4.6 to 7.1%). All aged alloys exhibited high corrosion resistance in 5.7% NaCl + 0.3% H2O2 water solution, with Zr-containing variants showing a lower corrosion rate and better pitting resistance. The study confirms the potential of tuning Sc/Zr ratios in Al–Zn–Ca alloys to achieve a favorable balance of strength, ductility, thermal conductivity, and corrosion resistance.
Al–Zn–Ca alloys are good candidates for industrial electronics and electric vehicles due to their high thermal conductivity, castability, and corrosion resistance, but their strength requires improvement. This study investigates how Sc and Zr additions affect the microstructure, thermal, mechanical, and corrosion properties of an Al–3wt%Zn–3wt%Ca base alloy. Microstructural analysis showed that substituting Sc with Zr did not drastically alter the phase composition but changed the elemental distribution: Sc was uniform, while Zr segregated to dendritic cores. Zr addition also refined the grain size from 488 to 338 μm. An optimal aging treatment at 300 °C for 3 hours was established, which enhanced hardness for all alloys via precipitation of Al3Sc/Al3(Sc,Zr) particles. However, this Zr substitution reduced thermal conductivity (from 184.7 to 168.0 W/mK) and ultimate tensile strength (from 269 to 206 MPa), though it improved elongation at fracture (from 4.6 to 7.1%). All aged alloys exhibited high corrosion resistance in 5.7% NaCl + 0.3% H2O2 solution, with Zr-containing variants showing a lower corrosion rate and better pitting resistance. The study confirms the potential of tuning Sc/Zr ratios in Al–Zn–Ca alloys to achieve a favorable balance of strength, ductility, thermal conductivity, and corrosion resistance.
1 June 2026 in International Journal of Lightweight Materials and Manufacture