Titanium alloys are of significant value in aerospace, biomedical, and marine engineering applications due to their excellent specific strength and favorable biocompatibility. As a crucial interstitial solute, oxygen significantly influences the mechanical properties of titanium alloys. However, excessive oxygen content can lead to severe embrittlement and a significant reduction in ductility. This paper systematically reviews the mechanisms of microstructural evolution induced by oxygen in conventionally manufactured titanium alloys and their impact on mechanical properties, highlighting that conventional processes require complex post-treatments (PT) to achieve a balance between strength and plasticity. This assessment further explores the regulatory mechanisms of oxygen on the microstructure and mechanical properties of laser additive manufactured (LAM) titanium alloys, elucidating the fundamental phenomena regarding the oxygen–microstructure–property relationship. Finally, based on the current research progress, this paper provides an outlook on the future development directions and key research priorities in this field. This review offers valuable insights into the role of oxygen in titanium alloys and the development of high-performance titanium alloys.
In this study, crack-free M2 high-speed steel (HSS) was successfully fabricated by laser powder bed fusion (L-PBF) using a relatively high substrate preheating temperature of 260 °C. The influence of the resulting microstructure on the hardness and tensile properties along the build direction was thoroughly investigated. The results demonstrate that M2 HSS achieves a relative density of 99.6% when processed with a laser power of 280 W and a scanning speed of 0.8 m s−1. The microstructure predominantly consists of fine martensite, along with retained austenite, lower bainite, and a small quantity of eutectic carbide. With increasing build height (from 0 to 9 mm), the fraction of lower bainite decreases from 32.1 to 13.1%, while the austenite content increases from 0.9 to 29.1%. These microstructural changes lead to a gradual reduction in the material’s strength along the build direction. Specifically, the hardness and tensile strength decrease from 845 HV0.3 and 1520 MPa to 745 HV0.3 and 1251 MPa, respectively. Additionally, the elongation varies between 2.6% and 3.3% across the different build heights.
To address the strength–ductility trade-off in titanium alloys, a comparative study was conducted on Ti-6Al-4V (TC4) alloys fabricated by laser powder bed fusion (L-PBF) and electron beam powder bed fusion (EB-PBF). The L-PBF specimen primarily consisted of acicular α′ martensite with high residual stress. In contrast, the EB-PBF specimens, owing to a substrate preheating temperature of 740 °C and a reduced cooling rate (103~105 K/s), exhibited a stable and coarse α + β lamellar structure. Combined with the high oxygen content (0.24 wt.%) that provided solid-solution strengthening, this morphology enabled simultaneous attainment of a yield strength of 1120 ± 12 MPa and an elongation at fracture of 11.1 ± 1.3%. Notably, deformation-induced HCP→FCC phase transformation occurred in EB-PBF alloys, generating a dual-phase HCP/FCC structure that effectively accommodated plastic strain. These results highlight the superior potential of EB-PBF over L-PBF for fabricating titanium alloys with an exceptional strength–ductility synergy.
H13 tool steel is widely used in the hot work die industry owing to its excellent mechanical properties. However, the inherent anisotropy of its microstructural and mechanical properties during additive manufacturing (AM) via laser powder bed fusion (L-PBF) hinders its broader application. In the current study, Ce-containing and as-built samples were prepared in both vertical and horizontal directions, and their microstructures and tensile properties were investigated. Notably, the grain size of the vertical samples is approximately 2.7 μm, which is 19.2% smaller than that of the horizontal samples in L-PBF H13 steel. In addition, the retained austenite (RA) content in the vertical samples reaches as high as 19.7%, whereas in the horizontal samples, it is only 0.4%. After the addition of Ce, the columnar grains of the building direction (BD) samples transform into equiaxed grains. The RA content of the scanning direction (SD) samples and BD samples is 6.3% and 5.7%, respectively. The tensile test results further demonstrate that Ce-containing BD samples exhibit a tensile strength of 2025.3 MPa and an elongation of 17.3%, with the elongation difference between the two directions being only 0.2%. The addition of Ce reduces microstructural anisotropy, resulting in a significant decrease in the mechanical property anisotropy of the formed parts.