Lucien Reclaru

Prof. Lucien Reclaru

Consultant Scientific, Neuchâtel, Switzerland
orcid

Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
21 September 2020 in Materials
Verified
Journal Article
Open access
PDF file
Lucien ReclaruLucien Reclaru
Lucien Reclaru
Lavinia Cosmina ArdeleanLavinia Cosmina Ardelean
Lavinia Cosmina Ardelean
Although called stainless steels, austenitic steels are sensitive to localized corrosion, namely pitting, crevice, and intergranular form. Seventeen grades of steel were tested for localized corrosion. Steels were also tested in general corrosion and in galvanic couplings (steels–precious alloys) used in watchmaking applications. The evaluations have been carried out in accordance with the ASTM standards which specifically concern the forms of corrosion namely, general (B117-97, salt fog test), pitting (G48-11, FeCl3), crevice (F746-87) and intergranular (A262-15, Strauss chemical test and G108-94, Electrochemical potentiodynamic reactivation test). All tests revealed sensitivity to corrosion. We have noticed that the transverse face is clearly more sensitive than the longitudinal face, in the direction of rolling process. The same conclusion has been drawn from the tests of nickel release. It should be pointed out that, despite the fact that the grade of steel is in conformity with the classification standards, the behavior is very different from one manufacturer to another, due to parameters dependent on the production process, such as casting volume, alloying additions, and deoxidizing agents. The quantities of nickel released are related to the operations involved in the manufacturing process. Heat treatments reduce the quantities of nickel released. The surface state has little influence on the release. The hardening procedures increase the quantities of nickel released. The quantities of released nickel are influenced by the inclusionary state and the existence of the secondary phases in the steel structure. Another aspect is related to the strong dispersion of results concerning nickel release and corrosion behavior of raw materials.

3 September 2019 in Materials
Verified
Journal Article
Open access
PDF file
Florina IonescuFlorina Ionescu
Florina Ionescu
Lucien ReclaruLucien Reclaru
Lucien Reclaru
Lavinia Cosmina ArdeleanLavinia Cosmina Ardelean
Lavinia Cosmina Ardelean
ABAndreas Blatter
Andreas Blatter
The evaluation of the biological safety and degradation of materials is quite important for risk assessment in various biomedical applications. In this study, two procedures were followed to characterize the corrosion resistance of different Ti-based alloys. The first one consisted of performing specific electrochemical tests (open circuit potential, linear resistance polarization, Tafel plots, potentiodynamic polarization) in order to highlight their behavior to the general and localized corrosion. The static and dynamic fatigue cycles combined with crevice corrosion conducted on a new prototype have completed the study. The second procedure followed was a cations extraction investigation (by inductively coupled plasma mass spectrometry) in order to verify the ionic permeability of the oxides layers formed on the surfaces. Optical and scanning electron microscopy were used for surface analysis. It was noticed that in these two electrolytes, the bulk Ti-based alloys presented an almost similar general corrosion behavior. The small differences of behavior for Ti6Al4V scaffolds were correlated to the surface oxidation and roughness (owing to the selective laser melting process). The Ti alloys presented no traces of localized corrosion at the end of the test. The fatigue cycles revealed that a strong and adhesive oxides film was formed during the static cycles (difficult to remove even during the depassivation steps). The concentration of cations released was at the detection limit, revealing very good passivation films, in adequacy with the all the other results.

5 April 2020 in Materials
Verified
Journal Article
Open access
PDF file
Lucien ReclaruLucien Reclaru
Lucien Reclaru
Lavinia Cosmina ArdeleanLavinia Cosmina Ardelean
Lavinia Cosmina Ardelean
CMCatalin Adrian Miu
Catalin Adrian Miu
AGAlexandru Florian Grecu
Alexandru Florian Grecu
Generally speaking, ceramic materials are insensitive to corrosion, compared to most other materials. The present study questions the fact that ceramics are inert. Two major aspects are to be considered: the stability of zirconia over time, the stable tetragonal phase transforming into an unstable monoclinic form; the multitude of manufacturing methods, using various additives, sintering additives, oxides mixing, impurities, grain boundaries, and porosities which strongly influence the corrosion behavior and chemical degradation. In case of the investigated ceramics two paths were pursued:a) Dissolutions of ceramics in a mixture of HNO3 60% and HF 40% ultrapure medium.b) Release of cations from ceramics in various mediums:dental bioceramics in a 0.07 M HCl medium and a 0.1% NaF+0.1% KF medium; ceramics used in jewelry and watchmaking applications in a HCl 0.07 M medium and an artificial sweat medium. By inductively coupled plasma-optical emission spectrometry/mass spectrometry (ICP-OES/MS), traces of significant chemical elements were assessed: Hf, Cr, Y, As, Pb, Al, Fe, Cu, Se, Sb, La, Ni, Co, Sb, Ta, Te, Ba, Sm, Nb, Hg, Cd, Sr, As and Se. In ceramics used in jewelry and watchmaking applications the concentrations found vary from one ceramic to another, including toxic elements such as Te, Ba, As, Pb, Sm, Hg and Cd, therefore being technical zirconia ceramics which are not intended for the medical field. For ceramics used in jewelry and watchmaking applications a screening identification test for Ni, Co, Cu and Fe with strips of type Merckoquant® (Merck, Kenilworth, NJ, USA) was also performed. The obtained data prove that the zirconia ceramics in question are far from being “inert”.

11 August 2025 in Materials
Verified
Journal Article
Open access
PDF file
Lucien ReclaruLucien Reclaru
Lucien Reclaru
AGAlexandru Florian Grecu
Alexandru Florian Grecu
DGDaniela Florentina Grecu
Daniela Florentina Grecu
CLCristian Lungulescu
Cristian Lungulescu
DGDan Cristian Grecu
Dan Cristian Grecu
Styles are invasive medical devices that are visible on images and are used in several medical specialties, including cardiology, neurology, orthopaedics, anaesthesia, oto-rhino-laryngology (ENT), and dentistry. With their thin and flexible design, they allow for the optimal positioning and precise guidance of medical devices such as nerve stimulation, defibrillation, electrode positioning, and catheter insertion. Generally, they are made of stainless steel, offering a combination of rigidity and flexibility. The aim of this study is to evaluate the sensitivity of austenitic stainless steel 304L used for the manufacture of J-stylets in uniform, pitting, crevice, and intergranular corrosion. We follow the manufacturing process step by step in order to analyse the risks of corrosion sensitisation and the cumulative effects of various forms of degradation, which could lead to a significant release of metal cations. Another objective of this study is to determine the optimal heat treatment temperature to minimise sensitivity to the intergranular corrosion of 304L steel. Uniform corrosion: Two samples were taken at each stage of the manufacturing process (eight steps in total), in the form of rods. After one hour of immersion, potentiodynamic polarisation curves were plotted up to ±400 mV vs. SCE. A coulometric analysis was also performed by integrating the anode zone between E (i = 0) and +400 mV vs. SCE. The values obtained by integration are expressed as mC/cm2. The test medium used was a simulated artificial plasma solution (9 g/L NaCl solution). Intergranular corrosion: (a) Chemical test: Thirty rod-shaped samples were tested, representing the eight manufacturing steps, as well as heat treatments at 500 °C, 620 °C, and 750 °C, in accordance with ASTM A262 (F method). (b) Electrochemical Potentiokinetic Reactivation (EPR) according to ASTM G108–94 (2015). Two samples were tested for each condition: without heat treatment and after treatments at 500 °C, 620 °C, and 750 °C. Release of cations: The release of metal ions was evaluated in the following two media: artificial sweat, according to EN 1811:2011+A1:2015, and bone plasma, according to the Fitton-Jackson and Burks-Peck method. Six samples that had been heat-treated at 500 °C for one hour were analysed. Results, discussions: (a) Analysis of the polarisation curves revealed significant disturbances in the heat treatment steps, as well as the μC/cm2 quantities, which were between 150,000 and 400,000 compared to only 40–180 for the other manufacturing steps; (b) Electrochemical Potentiokinetic reactivation (EPR) tests indicated that the temperature of 500 °C was a good choice to limit 304L steel sensitisation in intergranular corrosion; and (c) the quantities of cations released in EN 1811 sweat were of the order of a few μg/cm2 week, as for Fe: 2.31, Cr: 0.05, and Ni: 0.12.

13 April 2021 in Coatings
Verified
Journal Article
Open access
PDF file
Lucien ReclaruLucien Reclaru
Lucien Reclaru
Lavinia Cosmina ArdeleanLavinia Cosmina Ardelean
Lavinia Cosmina Ardelean
In the manufacturing of hypotubes for coronary applications, austenitic steels of types 304, 304, or 316 L are being used. The manufacturing process involves bending steel strips into tubes and the continuous longitudinal welding of the tubes. Manufacturing also includes heat treatments and stretching operations to achieve an external/internal diameter of 0.35/0.23 mm, with a tolerance of +/− 0.01 mm. Austenitic steels are sensitive to localized corrosion (pitting, crevice, and intergranular) that results from the welding process and various heat treatments. An extremely important step is the cleaning and the internal and external passivation of the hypotube surface. During patient interventions, there is a high risk of metal cations being released in contact with human blood. The aim of this study was to evaluate the state of passivation and corrosion resistance by using electrochemical methods and specific intergranular corrosion tests (the Strauss test). There were difficulties in passivating the hypotubes and assessing the corrosion phenomena in the interior of the tubes. Assessments were made by plotting the open circuit potential curves and exploring the polarization curves in the Tafel domain range of −50 mV vs. Ecorr (redox potential) and +150 mV vs. saturated calomel electrode (SCE, reference micro-electrode) for both the external and the internal surfaces of the hypotubes. The tested hypotubes did not exhibit intergranular corrosion, as mass losses were low and, in general, close to the limit of the analytical balance. Electrochemical techniques made the differentiation of the passivation state of the tested hypotubes possible. The measured currents were of the order of nano–pico amperes, and the quantities of electrical charges consumed for corrosion were of the order of micro–nano coulombs.

22 December 2022 in Coatings
Verified
Journal Article
Open access
PDF file
Lucien ReclaruLucien Reclaru
Lucien Reclaru
Nine grades of steel from different European steelmakers, namely 304L, 316L, and 904L, were evaluated. The austenitic steels studied are used in the manufacture of watch straps. The evaluations have been carried out in accordance with the ASTM standards which specifically concern the forms of corrosion, pitting (G48-11, FeCl3), intergranular (A262-15, Strauss method) test and Tuccillo–Nielsen test. The polarization electrochemical test on link watch straps was implemented by the microelectrode technique. Stress corrosion has also been investigated in the assembly of laser welded pin and link. It should be noted that, despite the fact that the grade of steel is in conformity with the classification standards, we note that the corrosion behavior is very different from one steelmaker to another. There are parameters that can change the quality of steel such as the technology process, casting volume, deoxidizers’ addition, remelted steel process and traces of pollutants. In consequence, we observe an extensive dispersion of results concerning nickel release, according to the EN 1811 European legislation regarding the protection of the population’s health, specifically relating to skin contact. In conclusion, steels DIN 1.4441 (316L Med) and DIN 1.4539 (904L) present a very good resistance to the morphologies of pitting and crevice corrosion. The 316L and 304L steel grades, also known as DIN 1.4435, DIN 1.4404 and DIN 1.4306, display a major difference in pitting and crevice corrosion behavior.