Out-of-autoclave (OoA) processing has emerged as a promising route for manufacturing high-performance polymer composites while reducing energy consumption and production complexity. The authors investigate the effect of curing temperature on the thermo-mechanical performances of carbon fiber-reinforced composites produced via resin infusion. Five laminates composed of six carbon fiber plies were arranged in a [90/0/45/−45/0/90] lay-up and infused with an epoxy resin cured at 25, 40, 50, 60, and 70 °C. The influence of the processed temperatures of the mechanical properties was evaluated through tensile and three-point bending tests, whereas thermal performance was analyzed using Heat Deflection Temperature (HDT) measurements and differential scanning calorimetry (DSC). The results demonstrate an improvement in stiffness, strength, and HDT with increasing the curing temperature, with the 40–50 °C range yielding the most balanced enhancement in mechanical and thermal responses. DSC analyses confirm that higher curing temperatures promote a more complete crosslinking reaction, consistent with the improved laminate performance. Overall, the findings highlight the critical role of controlled thermal curing in optimizing OoA polymer composite systems and support their suitability for energy-efficient applications.
Carbon-fiber-reinforced polymer (CFRP) composites fabricated with bio-based epoxy resins represent a promising approach for sustainable lightweight structures produced by out-of-autoclave (OoA) technologies. The curing schedule influences the state of the epoxy matrix and, consequently, can affect the fiber–matrix interaction and laminate performance. This study investigates the effect of practical curing conditions on 2 × 2 twill woven carbon fiber laminates fabricated by vacuum infusion using a commercially available bio-based epoxy resin IB2. The manufacturer’s recommended room-temperature conditions (25 °C for 24 h) were compared with accelerated mold heating schedules at 40, 50, 60, and 70 °C for 12 h. The laminates were characterized by three-point tensile and flexural tests, heat deflection temperature (HDT) measurements, differential scanning calorimetry (DSC), and SEM fractography. The tensile response showed limited sensitivity to the investigated curing conditions, with mean tensile strengths ranging from 634.01 to 672.95 MPa; T60 exhibited the highest mean numerical tensile strength (672.95 ± 53.60 MPa) and tensile modulus (53.39 ± 11.53 GPa), although the differences were small relative to the experimental spread. In contrast, the flexural response was more sensitive to the processing conditions. T70 exhibited the highest average flexural strength (980.60 ± 129.03 MPa), strain at maximum flexural stress, and strain energy density to maximum stress (8.75 ± 1.89 MJ/m3). The heat deflection temperature (HDT) systematically increased from 65.20 °C for T25 to 85.83 °C for T70. DSC revealed clear differences in the calorimetric response after curing during the first heating cycle, while the glass transition temperatures at the middle of the second heating occupied a relatively narrow range of 80.9–85.6 °C. SEM fractography revealed mixed tensile failure mechanisms related to fibers, matrix, and interface under all curing conditions. Overall, the results demonstrate that accelerated 12 h heated mold programs can reduce cure time while maintaining tensile performance generally comparable to the 24 h room-temperature IB2 reference condition and providing higher average flexural performance and thermal deformation resistance under load. These findings establish processing–property relationships relevant to the development of biomass-based CFRP OoA laminates for lightweight aerospace applications.
Carbon-fiber-reinforced polymer (CFRP) composites are widely used in lightweight aerospace structures because their mechanical performance can be adapted to different structural requirements through appropriate manufacturing conditions. This study investigates the influence of curing temperature applied using temperature-controlled heated molds on the mechanical and thermo-mechanical behavior of vacuum-infused CFRP laminates manufactured with an IN2 epoxy infusion resin. Laminates were cured at room temperature (25 °C) and at 40, 50, 60, and 70 °C using heated molds. Their performance was evaluated by tensile testing, three-point bending, and heat deflection temperature (HDT) measurements. The highest tensile strength (675.06 MPa) was obtained for laminates cured at 40 °C, whereas increasing the curing temperature beyond this value did not provide further improvement in tensile performance. The highest flexural stress at the first peak (983.36 MPa) and flexural modulus (67.17 GPa) were obtained for laminates cured at 70 °C, while the highest energy absorption during bending (0.57 J) was measured for laminates cured at 40 °C. The HDT increased from 59.77 °C for room-temperature curing to 87.60 °C for laminates cured at 70 °C, indicating improved thermo-mechanical stability with increasing curing temperature. The results indicate that no single curing temperature simultaneously maximized the tensile, flexural, and thermo-mechanical properties. Instead, the optimum curing temperature depended on the specific mechanical and thermo-mechanical requirements of the intended application. The results further indicate that controlling the temperature of heated molds during manufacturing provided a practical approach for tailoring the mechanical and thermo-mechanical performance of CFRP laminates without modifying the reinforcement architecture, laminate stacking sequence, or constituent materials.