Aircraft icing can substantially alter leading-edge geometry and degrade aerodynamic performance, highlighting the need for computationally efficient prediction methods during preliminary aircraft design. This study presents a two-dimensional reduced-order framework for airfoil ice-accretion prediction that couples a Hess–Smith potential-flow solver with Lagrangian droplet tracking, surface collection-efficiency reconstruction, a low-order freezing model, and an iterative geometry-update procedure. After each ice-accretion increment, the aerodynamic flow field and droplet trajectories are recomputed over the updated geometry, thereby capturing the coupled effects of ice growth, local flow acceleration, and downstream droplet impingement. A convergence study was performed to establish suitable surface and particle discretization. The predictive capability of the framework was assessed against four experimental NACA 23012 ice-accretion geometries representing streamwise and roughness-dominated configurations. The numerical predictions reproduced the location, extent, and principal morphological characteristics of the measured leading-edge deposits. Parametric investigations showed that the collection-efficiency distribution is governed primarily by the angle of attack, median volumetric diameter, and freestream velocity, whereas the maximum ice thickness is controlled predominantly by liquid water content and ambient temperature. Two-parameter response maps further revealed nonlinear interactions among droplet inertia, aerodynamic transport, incident water flux, freezing conditions, and geometry evolution. The proposed framework provides a practical, low-cost tool for preliminary icing assessment, sensitivity analysis, and rapid screening of atmospheric and operating conditions prior to higher-fidelity investigation.
Carbon-fiber-reinforced polymer (CFRP) composites are widely used in lightweight aerospace structures because their mechanical performance can be adapted to different structural requirements through appropriate manufacturing conditions. This study investigates the influence of curing temperature applied using temperature-controlled heated molds on the mechanical and thermo-mechanical behavior of vacuum-infused CFRP laminates manufactured with an IN2 epoxy infusion resin. Laminates were cured at room temperature (25 °C) and at 40, 50, 60, and 70 °C using heated molds. Their performance was evaluated by tensile testing, three-point bending, and heat deflection temperature (HDT) measurements. The highest tensile strength (675.06 MPa) was obtained for laminates cured at 40 °C, whereas increasing the curing temperature beyond this value did not provide further improvement in tensile performance. The highest flexural stress at the first peak (983.36 MPa) and flexural modulus (67.17 GPa) were obtained for laminates cured at 70 °C, while the highest energy absorption during bending (0.57 J) was measured for laminates cured at 40 °C. The HDT increased from 59.77 °C for room-temperature curing to 87.60 °C for laminates cured at 70 °C, indicating improved thermo-mechanical stability with increasing curing temperature. The results indicate that no single curing temperature simultaneously maximized the tensile, flexural, and thermo-mechanical properties. Instead, the optimum curing temperature depended on the specific mechanical and thermo-mechanical requirements of the intended application. The results further indicate that controlling the temperature of heated molds during manufacturing provided a practical approach for tailoring the mechanical and thermo-mechanical performance of CFRP laminates without modifying the reinforcement architecture, laminate stacking sequence, or constituent materials.