In order to explore the influence of the types of waste gypsum on the properties of alkali slag cement, fluorogypsum (FG) and flue-gas desulfurization (FGD) gypsum were comparatively investigated. Moreover, the action mechanisms of FG and FGD gypsum on the properties of alkali slag cement were analyzed. The results show that both the FG and FGD gypsum prolonged the setting time of the alkali slag cement paste. However, the prolongation effect of FG was more pronounced than the FGD gypsum. When the compressive strength was maximum, the contents of FG and FGD gypsum were 5 and 6 wt.%, respectively. At 3 and 28 days, compared to the control sample, the compressive strengths increased by 59.3% and 24.3%, and 66.9% and 33.9%, respectively. Furthermore, the XRD, TG-DTA and SEM-EDS results showed that, with the increase in the contents of FG and FGD gypsum, ettringite was more easily produced and the hydration products were more abundant in the system. The greater the gypsum content of the paste, the less accumulated was the heat of hydration. The change of micro-structure caused by the formation of ettringite was the main reason for the difference in the properties of cement.
To study the strengthening mechanism and effect underlying the reinforcement of a fractured rock mass with grouting, compressive shear tests were conducted with an RMT-150B rock mechanics test system. Prefabricated structural surfaces were strengthened with a new inorganic dual-liquid grouting material at five water–cement ratios (0.6–1.5). The effects of these water–cement ratios of the grouting on the deformation, strength, and failure characteristics of the prefabricated structural surface were analyzed. The results show that reinforcement with grouting significantly influenced the bearing capacity of the structural surface. The shear strength of the structure was significantly improved and the deformation resistance of the structural surface was enhanced. The shear stress–displacement curves, generated in compressive shear tests of the grouting-reinforced structures, were all nonlinear. The shearing process comprised three stages: elasticity, yield, and failure. Decreasing the water–cement ratio of the grouting material weakened the plasticity of the grouted structural surface and enhanced its brittleness. The deformation type changed from plastic slip to brittle shear. The shear strength, cohesion, and angle of internal friction of the grouting-reinforced structural surface increased with decreasing water–cement ratio.
An RMT-150B electrohydraulic servo testing system was used to perform uniaxial compression and uniaxial grading relaxation (creep) tests. The deformation, strength, and failure characteristics of the progressive failure process of coal samples under three loading modes were analyzed. The analysis results show that the prepeak stress-strain curve of the coal samples and the load relationships are not clear and that the whole compression process of coal still showed compression, elastic, yielding, and failure stages. The local stress drop characteristics during our relaxation creep grading tests showed no clear peak value and showed a yield curve with the shape of a conventional single plateau. The values of the mechanical parameters of axial compression were significantly higher than those obtained in the grade relaxation (creep) tests, which showed the mechanical parameters of coal samples with aging characteristics. In the relaxation (creep) tests, when the stress ratio was less than 70%, the relaxation (creep) characteristics of the sample were not clear. When the ratio of stress relaxation (creep) was more than 70% in the relaxation (creep) tests during displacement (stress) with a constant relaxation (creep) over the duration of the test, the evolution, development, and convergence of microcracks in the coal samples were observed. Relaxation (creep) stress was higher, failure duration was shorter, and the duration of failure was longer. For fully mechanized coal faces, increasing the support resistance and timely moving the support after coal cutting may prevent rib spalling accidents by reducing coal stress and exposure time in the front of the working face. Additionally, routine uniaxial compressive failures showed a simple form, having a clear tension-shear dual rupture surface. The staged relaxation creep failure testing of coal is more complex. The entire coal samples were divided into many thin-sheet debris via gradual collapse and shedding, and the number of cracks increased significantly, showing evident lateral expansion characteristics that are similar to the rib spalling characteristics in high coal mining working faces.
This research presents the grouting method of preventing rib sloughage which severely impacts mine safety and longwall retreat speed in thick coal seam with numerical simulation and laboratory tests. Based on the analysis of the plastic failure mode of five types of coal seam, roof strata ahead of the longwall face, and fractures developed in the coal seam, the following results are drawn, the range and degree of plastic failure generated in the coal seam and roof strata ahead of the longwall face gradually decreased as the coal mass strength increased; the grouting boreholes are essentially laid out within the coal rib instead of the roof. For a particular case of a coal mine in Shanxi province, a novel cement-based material was grouted, which fulfilled the reinforcement requirements under the tectonic stress regions and front abutment zones. Besides, the grouting borehole construction requested predrilled boreholes, full borehole intubation, lengthened hole sealing, and multiple-step drilling and grouting. This study can provide a theoretical framework of a design overview and practical basis for similar mining conditions in other coalfields.
High-flow low-expansion backfill materials have been developed to improve difficult slurry pipeline transport and poor roof-contact effect of many filling materials. The fly ash content was fixed at 80%, with 8.5% - 9.5% mineral powder content, 8.5% - 9.5% lime, 2% - 3% desulfurized gypsum, 0.9% - 1.2% sodium carbonate, and 0.01% - 0.02% aluminum powder content. The prepared backfill material processed good fluidity, with the expansion rate of the hardened material reaching 2% - 3%, and compressive strength on 90 d reaching 4 MPa—5.5 MPa. SEM observations indicated that as the aluminum content increased, ettringite on bubble walls transformed from a fine-needle to needle-rod shape. Secondly, the hydration products of the system were mainly hydrated calcium silicate gel and ettringite, which interconnected and promoted the formation of the structure. The backfill material has extensive sources of raw materials, low cost, simple filling process, and good filling effect.