Additively manufactured (AM) and wrought 316L stainless steels were irradiated with 2 MeV protons at 360 °C. Depth-resolved void swelling was quantified using cross-sectional transmission electron microscopy, with a safe-zone analysis applied to exclude near-surface and proton-range artifacts. The AM 316L exhibits significantly lower swelling than the wrought alloy. Swelling in the AM material is characterized by larger voids but a much lower void number density, whereas the wrought alloy develops smaller voids at a substantially higher density. The two alloys also display distinct dependences on local damage: in AM 316L, void size increases with local dpa while the void density remains nearly constant, whereas in wrought 316L, the void size is approximately constant and the void density increases with local dpa. These trends indicate that AM 316L has already entered a void growth-dominated regime, while wrought 316L remains in a void-nucleation-dominated regime. The reduced swelling in the AM alloy is attributed to more effective defect-recombination sinks and/or reduced vacancy mobility associated with the AM microstructure. These findings provide important insight for the evaluation and optimization of AM 316L alloys for nuclear industry applications.
Additively manufactured (AM) 316L stainless steel fabricated by laser powder bed fusion was irradiated with 5 MeV Fe self-ions to 50 peak displacements per atom at 600 °C to evaluate its swelling resistance in reactor-relevant environments. Cross-sectional transmission electron microscopy (TEM) revealed large voids with diameters up to 140 nm that were preferentially aligned rather than randomly distributed. The spacing between adjacent void strings was approximately 500 nm, matching the cellular wall structure present prior to irradiation. It is hypothesized that the high dislocation density associated with these walls acts as a strong yet biased sink for interstitials, promoting local vacancy accumulation and enhanced void formation. This facilitated nucleation also reduces the influence of injected interstitials, resulting in a wider safe analysis zone than typically observed during heavy-ion irradiation. Swelling measurements extracted from this region show an approximately linear dependence on local damage level, corresponding to a swelling rate of ~1% per dpa with little or no incubation period. The results indicate that the cellular structures play an important role in void swelling. The results demonstrate that the retained cellular structure plays a dominant role in void swelling evolution in AM 316L stainless steel. Therefore, post-build stress-relief treatments should be carefully optimized to reduce cellular dislocation density and enhance the swelling resistance of AM 316L for nuclear reactor applications.