Concrete is one of the most widely used construction materials globally, but it presents a critical vulnerability to high temperatures, which commonly manifests through explosive spalling. The incorporation of fibres has emerged as one of the most effective solutions to mitigate this problem. However, the comprehensive understanding of thermal degradation, hot-state flexural behaviour, the fibre-matrix interface, and the long-term viscoelastic response of fibre reinforced concrete remain subjects of scientific interest. The main objective of this doctoral thesis is to evaluate the mechanical, microstructural, and dimensional behaviour of different fibre reinforced concrete mixtures following their exposure to high temperatures and under sustained loads. A control concrete and mixtures reinforced with steel, polyolefin, and polypropylene fibres, as well as a hybrid combination subjected to severe thermal cycles of up to eight hundred and twenty-five degrees Celsius, were analysed, alongside long-term creep tests and hot-state flexural tests. The experimental results revealed a clear differentiation in the failure modes. Concretes without polymeric reinforcement suffered a violent failure due to spalling at internal temperatures close to two hundred degrees Celsius. Conversely, all mixtures containing polymeric fibres and the hybrid combination completely mitigated this phenomenon. In compressive strength tests, an unusual phenomenon of strength gain was observed in the polypropylene and hybrid mixtures after being subjected to four hundred and fifty degrees Celsius, attributed to a thermal post-curing effect. Thermogravimetric analysis demonstrated that the loss of strength at higher temperatures is due to the destruction of the main hydrated phases, calcium silicate hydrate gel and portlandite, coupled with the inelastic expansion of quartz. Regarding structural behaviour, hot-state flexural tests showed that the hybrid mixture lost its strain-hardening behaviour from one hundred and thirty degrees Celsius, giving way to strain-softening. Nevertheless, it was demonstrated that the steel fibres present in this mixture managed to govern the hot residual branch, maintaining significant toughness and preventing the brittle collapse of the element. To understand this phenomenon at a micromechanical level, fibres were extracted from the tested specimens and analysed. This study revealed that the rotation of the crack faces during bending induced asymmetrical friction during the pull-out stage, concentrating severe wear that degraded the surface embossing or roughness of the fibre, a deterioration exacerbated by the thermal softening of the polymer as it approached its melting point, justifying the loss of its anchorage capacity. Finally, data collection from creep tests over twenty-two months allowed for the characterization of the behaviour of creep and shrinkage deformations. Considering the results, evidence shows that the use of polymeric fibres constitutes a strategy to prevent collapse due to explosive spalling in high temperature situations. Experimental data suggest that the incorporation of hybrid reinforcement provides a good thermomechanical balance. In this reinforcement system, evidence suggests that the polyolefin fibre plays the role of an internal pressure relief network, while steel fibres take over the structural response in the hot state, providing a residual ductility that has not been obtained with the isolated use of polymeric fibres. Ultimately, this research contributes to the comprehensive knowledge of the behaviour of fibres-reinforced concretes exposed to high temperatures and time-dependent deformations. RESUMEN El hormigón es uno de los materiales de construcción más utilizado a nivel global, pero presenta una vulnerabilidad crítica frente a elevadas temperaturas la cual se manifiesta comúnmente mediante un desprendimiento explosivo o spalling. La incorporación de fibras se ha posicionado como una de las soluciones más eficaces para mitigar este problema. Sin embargo, la comprensión integral de la degradación térmica, el comportamiento a flexotracción en estado caliente, la interfaz fibra matriz y respuesta viscoelástica a largo plazo del hormigón reforzado con fibras siguen siendo temas de interés científico. El objetivo principal de esta tesis doctoral es evaluar el comportamiento mecánico, microestructural y dimensional de diferentes mezclas de hormigón reforzado con fibras tras su exposición a elevadas temperaturas y bajo cargas sostenidas. Se analizó un hormigón de control y reforzados con fibras de acero, poliolefina, polipropileno y combinación híbrida sometida a ciclos térmicos severos de hasta ochocientos veinticinco grados Celsius, así como también ensayos de fluencia y ensayos de flexotracción en caliente. Los resultados experimentales revelaron una diferenciación clara en los modos de fallo. Los hormigones sin refuerzo polimérico sufrieron un fallo violento por spalling a temperaturas internas cercanas a los doscientos grados Celsius. Por el contrario, todas las mezclas con fibras poliméricas y combinación híbrida mitigaron completamente este fenómeno. A nivel de compresión, se observó un fenómeno inusual de ganancia de resistencia en las mezclas con polipropileno e híbrida después de ser sometidas a cuatrocientos cincuenta grados Celsius, atribuido a un efecto de post curado térmico. El análisis termogravimétrico demostró que la pérdida de resistencia a mayores temperaturas se debe a la destrucción de las fases hidratadas principales, el gel silicato de calcio hidratado y la portlandita, sumada a la expansión inelástica del cuarzo. En cuanto al comportamiento estructural, los ensayos de flexotracción en estado caliente...