Demet Zalaoglu

Dr. Demet Zalaoglu

orcid

Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 October 2025 in Ceramics International
Verified
Journal Article
Closed access
Emre ÖzerEmre Özer
Emre Özer
DZDemet Zalaoglu
Demet Zalaoglu
MAMehmet Ayvaz
Mehmet Ayvaz
MÜMustafa Übeyli
Mustafa Übeyli
UAUmut Aksu
Umut Aksu
MEMusa Eryılmaz
Musa Eryılmaz

5 March 2025 in Surfaces and Interfaces
Verified
Journal Article
Closed access
SASafiye İpEk Ayvaz
Safiye İpEk Ayvaz
DZDemet Zalaoglu
Demet Zalaoglu
Emre ÖzerEmre Özer
Emre Özer
ABAli İhSan Bahçepınar
Ali İhSan Bahçepınar
İAİbrahim Aydın
İbrahim Aydın

19 January 2026 in Materials Testing
Verified
Journal Article
Closed access
MAMehmet Ayvaz
Mehmet Ayvaz
Emre ÖzerEmre Özer
Emre Özer
DZDemet Zalaoglu
Demet Zalaoglu
MÜMustafa Übeyli
Mustafa Übeyli
UAUmut Aksu
Umut Aksu
MEMusa Eryılmaz
Musa Eryılmaz
Magnesium biocomposites reinforced with biocompatible ceramic particles are considered promising biomaterials for orthopedic applications due to their biodegradability and compatibility with bone regeneration. In addition to mechanical and corrosion performance, the in vitro wear behavior of these materials is critical for implant components subjected to frictional loading. In this study, the sliding wear behavior of Mg2Zn1Mn nano-biocomposites reinforced with hydroxyapatite (HA) and alumina (Al 2 O 3 ) nanoparticles was investigated under a 10 N load in both dry and simulated body fluid (SBF) environments. The influence of reinforcement content and sintering route (one-step and two-step) on wear performance was examined. The results revealed that wear losses were higher in SBF than in dry conditions, due to simultaneous corrosion-assisted wear, as well as the incorporation of 6 wt.% HA and Al 2 O 3 nanoparticles, together with two-step sintering, improved in vitro wear resistance by 33.9 %. Scanning electron microscopy analyses showed that abrasive and oxidative wear dominated under dry sliding conditions, whereas corrosive wear became the primary mechanism in SBF. These findings demonstrate that dual ceramic reinforcement significantly enhances the wear resistance of Mg2Zn1Mn biocomposites, particularly in physiological environments.

17 July 2023 in Journal of Boron
Verified
Journal Article
Open access
PDF file
MEMehmet Eker
Mehmet Eker
DZDemet Zalaoglu
Demet Zalaoglu
Bu çalışmada, toz metalurjisi yöntemi ile hazırlanan, farklı oranlarda (hacimce % 0, 10 ve 20) B4C parçacık takviyeli Al-%10Cu ana yapılı kompozit malzemenin sinterleme sonrası yoğunluğuna, takviye oranı, sıkıştırma basıncı ve sinterleme sıcaklığının etkisi incelenmiştir. Kompozit üretimi için yüksek saflıkta alaşım ve seramik tozları kullanılmış, elde edilen homojen karışım soğuk preste sıkıştırılmış ve tüp fırında sinterlenmiştir. Tayin edilen değişkenlerin sinterleme sonrası yoğunluğa etkisi Taguchi deney tasarımı yöntemi kullanılarak incelenmiştir. Bu amaç ile sürece en uygun Taguchi tasarımı olan, L9 ortogonal deney tasarımı seçilmiş ve deneyler bu matrise göre gerçekleştirilmiştir. Bu tasarım ile yapılan analizler sonucunda elde edilen S/N oranı yanıtlarına göre, sıkıştırma basıncının en yüksek etkiye, takviye oranının da görece düşük etkiye sahip olduğu gözlemlenmiştir. Taguchi deney tasarımı ve yapılan regresyon analizi sonucunda, oluşturulan regresyon modelinin ise %95 güven aralığın içinde olduğu sonucu elde edilmiştir.

25 June 2025 in Archives of Metallurgy and Materials
Verified
Journal Article
Open access
PDF file
ISI. Sarpkaya
I. Sarpkaya
Emre ÖzerEmre Özer
Emre Özer
DZDemet Zalaoglu
Demet Zalaoglu
MÜM. Übeyli
M. Übeyli
yusuf fedaiyusuf fedai
yusuf fedai
The machinability of aluminum hybrid composites (AHCs) can be enhanced by utilization of optimum composition and cutting parameters. In this study, the machinability of AHCs containing micron-sized TiB2 and B4C particles was investigated using the face milling operation with a double coated cemented carbide tool. The composites, fabricated via cold pressing and microwave sintering, were subjected to the face milling experiments using a CNC milling machine. The influence of hybrid reinforcement content, feed rate and cutting speed on tool wear and surface roughness was examined during the milling of these composites. After the machinability tests, the worn surface of inserts was examined by a scanning electron microscope to see the wear types. The reinforcement content and cutting speed were obtained to have a much greater effect on the machinability and surface roughness of the hybrid composites compared to the feed rate. Either increasing the feed rate or decreasing the cutting speed provided a larger amount of chip removal until the wear limit. Moreover, the feed rate was obtained to be more effective on the tool wear at lower cutting speeds and higher amounts of hybrid reinforcement.

8 July 2024 in Materials Testing
Verified
Journal Article
Closed access
OAOnur Altuntaş
Onur Altuntaş
Emre ÖzerEmre Özer
Emre Özer
DZDemet Zalaoglu
Demet Zalaoglu
MÜMustafa Übeyli
Mustafa Übeyli
In this paper, the welding quality of API 5L X60 steel pipes was investigated after the application of three different welding scenarios by applying submerged arc welding (SMAW), tungsten inert gas (TIG) and hybrid (TIG + SMAW) welding methods with an average heat input of ca. 1 kJ mm −1 for all passes. For this purpose, the ultrasonic and radiographic tests were done to detect possible discontinuities such as crack and porosity in the welding zones. In addition, the macro and microstructures of weld zones were made to examine different zones in terms of weld quality and phases. Moreover, the hardness, impact toughness and tensile tests were carried out to determine the mechanical properties of the weldments. The tensile strength of the pipe weldments was recorded to be ∼603, 610 and 625 MPa after the welding of pipes by SMAW, TIG + SMAW and TIG welding, respectively. In addition, the impact toughness of the welds was obtained to be 48, 76 and 66 J, for these welding methods, successively. According to the experimental findings, all three welding plans were successfully applied to the steel pipes and found to be suitable regarding the relevant international standards.