The incorporation of recycled metallurgical slags into refractory materials constitutes a promising approach to enhancing sustainability in the refractory industry. This study investigates the effect of vanadium-bearing slag aggregates as partial replacements for tabular alumina in castables and compares their behaviour with high-alumina and bauxite-based castables. Two vanadium-bearing slags with different mineralogical compositions were introduced in the 1–3 mm aggregate fraction with substitution up to 25 wt.%. Their effects on microstructure, thermo-mechanical performance, and corrosion resistance were evaluated. The introduction of vanadium-bearing slag significantly alters the microstructure of the castables, affecting their performance. Both slags displayed grains with higher porosity, microcracking, and heterogeneity compared with tabular alumina, but showed similarities to bauxite grains. Slag 1, enriched in calcium aluminate phases, provides limited mechanical strength but improved corrosion resistance due to improved bonding with the matrix. Slag 2, containing a higher spinel content, enhances mechanical strength, showing behaviour comparable with bauxite-based castables, particularly at 10 wt.% replacement. Vanadium is mainly present in metallic form and as Mg(Al,V)2O4 spinels in both slags. Upon firing, vanadium migrates toward the grain boundaries and reacts with the surrounding calcium aluminate phases to be incorporated in Ca(Al,V)2O4 and Ca(Al,V)4O7, while the spinel phase remains stable.
The incorporation of recycled metallurgical slags into refractory materials constitutes a promising approach to enhancing sustainability in the refractory industry. This study investigates the effect of vanadium-bearing slag aggregates as partial replace-ments for tabular alumina in castables and compares their behaviour with high-alumina and bauxite-based castables. Two vanadium-bearing slags with differ-ent mineralogical compositions were introduced in the 1-3 mm aggregate fraction with substitution up to 25 wt.%. Their effects on microstructure, thermo-mechanical performance and corrosion resistance were evaluated. The introduction of vanadi-um-bearing slag significantly alters the microstructure of the castables, affecting their performance. Both slags displayed grains with higher porosity, microcracking, and heterogeneity compared with tabular alumina, but show similarities with bauxite grains. Slag 1, enriched in calcium aluminate phases, provides limited mechanical strength but improved corrosion resistance due to improved bonding with the matrix. Slag 2, containing a higher spinel content, enhances mechanical strength, showing behaviour comparable to bauxite-based castables, particularly at 10 wt.% replacement. Vanadium is mainly present in metallic form and as Mg(Al,V)2O4 spinel in both slags. Upon firing, vanadium migrates toward grain boundaries and reacts with surround-ing calcium aluminate phases to be incorporated in Ca(Al,V)2O4 and Ca(Al,V)4O7, while the spinel phase remains stable.
7 November 2024 in International Journal of Ceramic Engineering & Science
Handling the massive quantities of by‐products from metallurgical processes has become a major concern in recent decades. Efforts to develop sustainable alternatives for these secondary resources are ongoing to achieve the transition to climate neutrality. This study has investigated the potential of employing vanadium‐bearing slag as a new value‐added binder in refractories, aiming to replace virgin raw materials. Two types of vanadium‐bearing slags from BOF, each containing <2 wt.% vanadium were studied. Low‐cement vanadium slag‐based castables were prepared by gradually substituting 0, 2.5, and 5 wt.% of the commercial calcium aluminate cements (Secar71 and CMA72) by the slags. The flow values of the mixes containing 5 wt.% of slag decrease significantly from about 90% to 30% after 30 min, showing poor ability to flow and thus are not considered as self‐flow castables. Castables containing 2.5 wt.% of slag present a cold crushing strength value, in the range of 71–116 MPa while values for castables containing 5 wt.% of slag fall into the range of 53–68 MPa due to the lower packing properties leading to higher porosity and reduce in strength. Similar observation was concluded for cold modulus of rupture. The micrographs of the samples containing both slag and cement show promising compatibility between the binder and aggregates after sintering at 1500°C. Overall, characteristics obtained with the samples containing slag show promising alternatives as a refractory lining.
28 February 2026 in Journal of the American Ceramic Society