Electrospinning is a widely used technique for fabricating nanomaterials with tailored morphology and functional properties. This study investigates how two fundamental process parameters—applied voltage and needle tip-to-collector distance—affect the spatial geometry and deposited mass of electrospun nanofiber mats in a top-down vertical electrospinning setup using a 10% (w/v) PVA solution prepared in deionized water. To support this hypothesis, both experimental measurements and 3D geometric modeling were performed to evaluate the area, perimeter, and deposited mass under different parameter combinations. Digital image analysis and cross-sectional reconstruction were applied to model nanofiber deposition. Regression and ANOVA analyses reveal that the tip-to-collector distance has a statistically significant impact on both area and perimeter of the electrospun nanofiber mat, while the applied voltage in the tested range (15–20 kV) has no significant effect. Interestingly, the total deposited mass shows no clear dependence on either parameter, likely due to startup irregularities or solution droplets.
Electrospun poly(vinyl alcohol) (PVA) nanofibrous mats containing Spirulina or Chlorella biomass were deposited directly onto a woven cotton fabric to produce fabric–nanomat composites. The effects of the microalgal species on the physicochemical properties of the electrospinning solutions, nanofiber morphology, nanomat development, surface porosity, and through-plane transport properties were comparatively investigated. The incorporation of either biomass increased the viscosity, electrical conductivity, and surface tension of the PVA solution, indicating interactions between the microalgal components and the polymer matrix. FTIR analysis showed that the nanomats largely retained the characteristic absorption bands of neat PVA, with minor spectral features consistent with the incorporated biomass. SEM observations revealed continuous, bead-free nanofibers without visible surface defects. The average fiber diameters were 192 ± 34 nm for PVA/Spirulina and 173 ± 39 nm for PVA/Chlorella. The PVA/Chlorella system produced thicker nanomats, whereas the PVA/Spirulina system exhibited greater projected-area expansion during prolonged electrospinning. Surface porosity was significantly higher for PVA/Spirulina nanomats (57.54 ± 1.34%) than for PVA/Chlorella nanomats (52.69 ± 1.49%). Correspondingly, the PVA/Spirulina composites exhibited higher air permeability, whereas both systems showed comparable relative water vapor permeability. These results demonstrate that the type of microalgal biomass influences nanomat development, morphology, porosity, and air permeability while having a limited effect on relative water vapor permeability, providing a basis for the development of functional textile and filtration-related materials.