Nano-FTIR and PeakForce quantitative nanomechanical mapping (PF QNM) are new AFM-based techniques that can be applied to plant tissues to get high-resolution spatial distribution of features that are unavailable from bulk characterization. This can be useful for finding changes to plant cell walls by processing technologies, mutations, or the environment. Three poplar hardwoods of varying recalcitrance and composition (high lignin, low lignin, and mutant) were investigated by nano-FTIR and PF QNM. Bulk characterization was carried out by conventional FTIR and NMR of isolated cellulose, hemicelluloses, and lignin. We found that in nano-FTIR spectra of secondary cell walls (SCW) and compound middle lamella (CML), 1162 and 1269 cm–1 could distinctly identify polysaccharides and lignin, respectively. Spatial variability in the content of polysaccharides and lignin was significantly larger in CML than SCW for all three poplars. Cellulose has a disordered structure in CML in comparison to SCW. PF QNM showed that SCW had a higher modulus of elasticity than CML due to the presence of crystalline cellulose in SCW. Differences in the physicochemical properties between the SCW and CML of plants can be probed at nanoscale by these techniques.
Bacterial cellulose (BC) film formation could be a critical issue in nanotechnology applications such as biomedical or smart materials products. In this research, purified pretreated BC was subjected to high intensity ultrasound (HIUS) and was investigated for the development of BC films. The morphological, structural and thermal properties of the obtained films were studied by using FE-SEM, AFM, FT-IR, XRD, TGA and DSC characterizations. Results showed that the most favorable purification treatment was the 0.01 M NaOH at 70°C for 2h under continuous stirring. The most suitable ultrasound operating conditions were found to be, 1cm distance of ultrasonic probe from the bottom of the beaker, submerged in cold water bath cooling around 12 ± 2°C. The power (25 W/cm(2)), time (30 min), BC concentration (0.1%w/w), amplitude (20 μm) and frequency (20 kHz) were maintained constant.
Alterations in the chemical composition of silver fir wood (Abies alba L.) during thermal treatment were investigated. The mass loss, extractives, saccharides, and lignin were determined. In both untreated and heat-treated wood, extractives were determined according to ASTM D1107-96, lignin content according to ASTM D1106-96, and saccharides by high-performance liquid chromatography. During the thermal treatment, mass loss and the chemical composition of the wood were found to change. The extractives content decreased up to 200 °C, and then increased at higher temperatures. The mass loss increased with increasing temperature and time of thermal treatment. A relative increase in lignin content and a decrease in saccharides were observed. The color of the wood was stable at temperatures up to 150 °C when treated up to 1 h. A change in color significantly depends on thermal energy intake above that level. Saccharides, color coordinates L* and b*, lignin, mass loss, temperature, and color change ΔE* strongly vary together. These investigated properties of fir wood set out the boundaries for high-temperature treatment and show potential for utilization of this species.