As an environmentally friendly natural polymer, citric acid-modified chitosan (CAMC) can effectively regulate the hydration and exothermic processes of cement-based materials. However, the influence of CAMC on the macroscopic properties of concrete and the optimal dosage are still unclear. This work systematically investigates the effects of CAMC on the mixing performance, mechanical properties, shrinkage performance, and durability of concrete. The results indicated that CAMC has a thickening effect and prolongs the setting time of concrete. CAMC has a negative impact on the early strength of concrete, but it is beneficial for the development of the subsequent strength of concrete. With the increase in CAMC content, the self-shrinkage rate of concrete samples decreased from 86.82 to 14.52 με. However, the CAMC-0.6% sample eventually expanded, with an expansion value of 78.49 με. Moreover, the long-term drying shrinkage rate was decreased from 551.46 to 401.94 με. Furthermore, low-dose CAMC can significantly reduce the diffusion coefficient of chloride ions, improve the impermeability and density of concrete, and thereby enhance the freeze–thaw cycle resistance of concrete.
The temperature stress caused by the large temperature difference is the main factor causing harmful cracks in large-volume concrete. The introduction of admixtures is beneficial to reduce the temperature difference inside and outside the large-volume concrete. This study investigated the mechanism of how citric acid-modified chitosan (CAMC) affects the hydration heat release process and hydration products of composite cementitious materials. Through methods such as hydration heat, X-ray diffraction (XRD), mercury intrusion porosimetry (MIP), scanning electron microscopy (SEM), and nuclear magnetic resonance (NMR), the mechanism of how CAMC controls the hydration heat release process and hydration products of composite cementitious materials was revealed. The results show that the addition of CAMC delayed the hydration process of cementitious materials without affecting the type of hydration products but affected the content of each phase of hydration products. As the hydration process proceeded, the total porosity of all samples decreased, the volume of large pores decreased, and the volume of small pores increased. As the content of CAMC increased, the pore diameter of the hardened paste gradually became smaller, the proportion of large pores decreased, and the later hydration microstructure became more dense. The increase in CAMC dosage resulted in a decrease in the peak intensity of Q2 in the paste, indicating that Al atoms in Q2 (1Al) existed in the form of Alcoordination, which proves that CAMC reduced its hydration degree and delayed cement hydration.
In the present study, the evolution of free water content in five different alkali-activated slag (AAS) systems was continuously monitored and compared using 1H low-field NMR. The alkali activators used were waterglass solutions with three different moduli (1.2, 1.4, and 1.6), sodium hydroxide solution, and sodium sulfate solution. The findings reveal that the type of activator significantly affected the dynamic changes in the relative free water content. Notably, an increase in free water content was observed in the early stages of hydration of all AAS systems except for those activated by sodium sulfate solution. Additionally, this study investigated the relationship between changes in free water content and hydration heat in the AAS systems, dividing the initial 24 h of AAS hydration into three stages. The results demonstrate that free water can serve as an effective probe for monitoring the hydration process in fresh AAS pastes, offering valuable insights alongside traditional thermal signals.
The primary objective of this study is to investigate the effect and mechanism of replacing limestone powder with red mud as a filler on asphalt aging resistance. The microstructure and porosity characteristics of limestone powder, Bayer process red mud, and sintered red mud were analyzed. Asphalt mastics were then prepared using these fillers. The effect of red mud on the aging resistance of asphalt was evaluated by comparing the conventional physical properties, rheological behavior, and functional groups of the asphalt mastics before and after aging. Fourier transform infrared spectroscopy (FTIR), gel permeation chromatography (GPC), and ultraviolet-visible spectroscopy (UV-Vis) were further employed to elucidate the underlying anti-aging mechanisms. The results indicate that the asphalt mastic containing 4% sintered red mud exhibits the strongest resistance to both thermo-oxidative and UV aging. It shows the lowest increments in softening point, viscosity aging index, and complex modulus aging index, with performance comparable to a commercial anti-aging agent. FTIR and GPC analyses reveal that sintered red mud selectively adsorbs light asphalt components, thereby inhibiting their conversion into heavier fractions during thermo-oxidative aging. UV-vis analysis demonstrates that sintered red mud provides effective UV shielding within the asphalt mastic, substantially mitigating UV-induced damage. In summary, the incorporation of 4% sintered red mud can significantly delay both thermo-oxidative and UV aging processes in asphalt mastics, thereby effectively enhancing the aging resistance of asphalt pavement.
Every year, a billion tires are discarded worldwide, with only a small percentage being recycled. This leads to significant environmental hazards, such as fire risks and improper disposal. Silty sand also presents technical challenges due to its poor shear strength, susceptibility to erosion, and low permeability. This study explores the incorporation of crumb rubber derived from waste tires into silty sand to enhance its mechanical properties. Crumb rubber particles of varying sizes (3–6 mm, 5–10 mm, and 10–20 mm) were mixed with silty sand at 0%, 3%, 6%, and 9% percentages, respectively. Triaxial compression tests of unconsolidated and consolidated undrained tests with cell pressures of 100, 300, and 500 kPa were conducted. The deviatoric stress, shear stress, and stiffness modulus were investigated. The results revealed that the addition of crumb rubber significantly increased the deviatoric and shear stresses, especially at particle sizes of 5–10 mm, with contents of 3%, 6%, and 9%. Additionally, the stiffness modulus was notably reduced in the mixture containing 6% crumb rubber tire. These findings suggest that incorporating crumb rubber tires into silty sand not only improves silty sand performance but also offers an environmentally sustainable approach to tire waste recycling, making it a viable strategy for silty sand stabilization in construction and geotechnical engineering performance.