The stabilization of waste sludge generated from various engineering projects to produce sludge solidified soil for use as subgrade fill is one of the effective approaches for the resource utilization of construction spoil. However, such solidified soils are typically characterized by relatively low stabilizer content and are subjected to long-term cyclic dynamic loading during their service life. In this study, typical sludge from the Ningbo region was used to prepare cement-stabilized soils with low cement content (4–7%). A series of dynamic triaxial tests under long-term cyclic loading were conducted to systematically investigate the evolution of dynamic strength, cumulative deformation, and initial dynamic elastic modulus. The test results revealed the following: (1) The cumulative deformation of the solidified soil exhibited either a “stable” or a “failure” pattern, with the transition governed by the critical dynamic load, which was strongly influenced by the cement content. (2) Increasing the cement content significantly enhanced the fatigue resistance of the solidified soil; when the content was increased from 4 to 6%, the fatigue life improved by up to 575%. (3) When the cement content exceeded 6%, the growth rates of both fatigue life and initial dynamic elastic modulus slowed markedly, indicating a clear phenomenon of diminishing marginal returns. This study identified 6–7% as the optimal economic range of cement content, achieving an optimal balance between dynamic stability and material cost. These findings provide critical design parameters and performance optimization references for the application of stabilized sludge in road engineering.
High-content cemented soils are critical for modern geotechnical technologies (e.g., pre-bored precast piles), yet their long-term durability remains underexplored. This study investigates the 28- to 365-day mechanical and microstructural evolution of high-content cemented silty clay under freshwater and seawater curing via UCS, SEM, MIP, and XRD. Under freshwater, cement content directly dictated strength, with the 8:2 mix reaching 24.31 MPa at 365 days. However, marginal efficiency analysis confirmed diminishing returns for excessive binder, establishing the 7:3 ratio as the optimal baseline. Seawater exposure induced a biphasic response: a 4.6% early strength gain at 28 days, followed by severe degradation (a 23.5% drop at 365 days). Concurrently, the failure mode shifted to macroscopic “pseudo-ductility,” with peak strain increasing from 2.37% to 3.04%. Crucially, a micro–macro inconsistency emerged: although seawater physically refined the pore structure (micropore proportion doubled to 30.2% at 90 days) via expansive salts filling mesopores, macroscopic strength declined. XRD confirmed this degradation coincides with severe long-term alkaline buffer (Ca(OH)2) depletion. Consequently, lifecycle durability assessments for high-binder marine systems must not rely solely on physical metrics like porosity, but adopt a coupled multi-factor framework prioritizing chemical stability.