The effects of the γ″-Ni3Nb phase on the mechanical properties of Inconel 718 superalloys, with standard heat treatment, hot isostatic pressing + solution treatment + aging, and hot isostatic pressing + direct aging, were characterized by morphological observation, X-ray diffraction, and tensile experiments. The results of the morphological observation revealed that many fine γ″ precipitates of ~26.49 ± 1.82 nm in mean size were formed in all samples. However, the relatively coarser γ″ precipitates formed in the grain boundaries were only observed in the sample treated with hot isostatic pressing + direct aging. The yield strengths of the hot isostatic pressing + direct aging sample at room temperature and at 650 °C both exhibited the maximum values about 993 ± 5.7 and 811 ± 12.6 MPa, respectively. The γ″ precipitate was considered to be the dominant strengthening phase in the sample according to the lattice misfits (ε) of γ/γ″. The strengthening mechanism of the samples can be explained as the coherency strain strengthening of fine γ″ precipitates. Moreover, due to the coarser γ″ precipitates in the grain boundaries, dislocation-cut ordered particle strengthening also occurred in the sample after hot isostatic pressing + direct aging treatment.
Along with the globalization of environmental problems and the rapid development of the field of nuclear technologies, the severe irradiation damage of materials has become a big issue, restricting the development of advanced nuclear reactor systems. Refractory high-entropy alloys (RHEAs) have the characteristics of a complex composition, a short-range order, and lattice distortion and possess a high phase stability, outstanding mechanical properties, and excellent irradiation resistance at elevated temperatures; thus, they are expected to be promising candidates for advanced nuclear reactors. This review summarizes the design, preparation, and irradiation resistance of irradiation-tolerant RHEAs. It encompasses a comprehensive analysis of various aspects, including the evolution of defects, changes in microstructure, and the degradation in properties. Furthermore, the challenges and insufficiently researched areas regarding these alloys are identified and discussed. Building on this foundation, the review also provides a forward-looking perspective, outlining potential avenues for future research.
Additive manufacturing provides an efficient way of producing metallic components with complex geometries. Their microstructure is substantially different to those from conventional processing, creating opportunities for manipulating the final microstructure and properties via heat treatment. Here, we demonstrate that as-built heterostructures in an Al-Zn-Mg-Cu-Nb alloy produced during the solidification of molten pools provide a driving force and additional Zener pinning sources for recrystallization. This creates a bimodal grain structure after solution treatment, causing additional hetero-deformation-induced strengthening and hardening. Coarse grains are found to promote work hardening and blunt the propagate of cracks during deformation, increasing ductility. Together with precipitation strengthening from a high number density nanoprecipitates, the simultaneous improvement of strength and ductility in a highly alloyed Al-Zn-Mg-Cu-Nb alloy is achieved. These results provide a simple strategy for the development of additively manufactured age-hardening alloys with improved strength and ductility for high performance structural applications.
Freckle defects usually appear on the surface of castings and industrial ingots during the directional solidification process and most of them are located near the interface between the shell mold and superalloys. Ceramic cores create more interfaces in the directionally solidified (DS) and single crystal (SX) hollow turbine blades. In order to investigate the location of freckle occurrence in superalloys, superalloy CM247 LC was directionally solidified in an industrial-sized Bridgman furnace. Instead of ceramic cores, Alumina tubes were used inside of the casting specimens. It was found that freckles occur not only on the casting external surfaces, but also appear near the internal interfaces between the ceramic core and superalloys. Meanwhile, the size, initial position, and area of freckle were investigated in various diameters of the specimens. The initial position of the freckle chain reduces when the diameter of the rods increase. Freckle area follows a linear relationship in various diameters and the average freckle fraction is 1.1% of cross sectional area of casting specimens. The flow of liquid metal near the interfaces was stronger than that in the interdendritic region in the mushy zone, and explained why freckle tends to occur on the outer or inner surfaces of castings. This new phenomenon suggests that freckles are more likely to occur on the outer or inner surfaces of the hollow turbine blades.
The dimensionless Niyama criterion was used to predict the formation of microporosity in nickel-based superalloy casting, which extended the model application from a simple plate casting to complex thin-wall superalloy casting. The physical characteristics of the superalloy were calculated by JMatPro software. The relation between the volume percentage of microporosity and the dimensionless Niyama values were constructed. Quantitative metallographic measurements of the microporosity of the practical thin-wall casting were carried out. The prediction agreed well with the experiment in general, except for some thick-wall sites in the casting.