Lignin, the second most abundant polymer, remains largely underutilized, with nearly 90% of industrial lignin being combusted for energy due to its low phenolic hydroxyl content and structural heterogeneity of conventional extraction methods. The present study proposes a synergistic extraction method integrating sequential hydrothermal and twin-screw extrusion pretreatment followed by aqueous ethanol organosolv extraction. Three pretreatment strategies—hydrothermal pretreatment, twin-screw extrusion pretreatment, and sequential hydrothermal and twin-screw extrusion pretreatment—were compared. The sequential pretreatment exhibited the most favorable performance. Upon organosolv extraction, a lignin extraction rate of 67.9% was achieved, representing a 20.8% increase over that of the raw material. Extensive β-O-4′ bond cleavage during the integrated process liberated phenolic hydroxyl groups. This elevated the total phenolic hydroxyl content to 3.43 mmol·g−1, representing a 63.3% increase relative to lignin derived from raw material. Concurrently, this bond cleavage yielded lignin with a narrower molecular weight distribution, indicating enhanced structural homogeneity. Additionally, cellulose retention after lignin extraction reached 88.9%. Mass-balance calculations indicated that 1000 g of raw material yielded 82.5 g of xylose and xylooligosaccharides, 148.2 g of highly active lignin, and cellulose-enriched solid residues, thereby facilitating the comprehensive utilization of the three primary components of lignocellulosic biomass.
6 October 2026 in Frontiers in Bioengineering and Biotechnology
This study aims to overcome the structural recalcitrance of lignocellulosic biomass and improve the economic viability of biorefineries. A multi-step sequential pretreatment strategy combining hydrothermal pretreatment, twin-screw extrusion, and deep eutectic solvent (DES) treatments was developed to effectively deconstruct poplar biomass while recovering high-quality lignin, xylooligosaccharides (XOS), and fermentable sugars.The results demonstrated that this integrated approach achieved exceptional pretreatment performance, with 89.7% delignification and 85.3% xylan removal. The strategy enabled near-complete cellulose enzymatic hydrolysis at a low enzyme loading (15 FPU/g) and achieved a 45.7% XOS yield. Furthermore, the process yielded high-purity lignin (99.9%) with an 81.5% recovery rate,characterized by reduced molecular weight, enhanced antioxidant activity (IC 50 = 56.16 mg/L), and a high phenolic hydroxyl content (2.81 mmol/g).This sequential pretreatment strategy exhibits significant potential for the integrated valorization of poplar biomass into fermentable monosaccharides, functional oligosaccharides, and antioxidant lignin derivatives, advancing the sustainability of lignocellulosic biorefineries.