Resource depletion and climate change have fostered sustainable initiatives in the waste management sector. Pyrolysis (Py) has emerged as an option for valorizing spent coffee grounds (SCG). In addition, inorganic compounds can have catalytic effects on the pyrolytic reaction of organic materials, increasing the char yield and porosity of biochar. This study investigates the slow pyrolysis of SCG using concentrated landfill leachate residue (CLLR) (1:1 wt%) as a pyrolitic additive due to its high salinity. Biochars were characterized based on their thermal behavior to discuss environmental benefits and potential applications. Slow-py experiments were conducted using a lab-scale pyrolizer, and thermal characterization was performed using TA Instruments, specifically the SDTQ600 model. Biochars were characterized by higher water contents and heating rates than those experienced by their feedstocks. It is suggested that the high metal content of CLLR could change the biochar’s thermal stability, decreasing its decomposition temperature. Values were 9.18 wt% and 18.11 MJ kg−1 and 23.25 wt% and 22.05 MJ kg−1 for biochars produced using SCG and SCG and CLLR (1:1 wt%), respectively. Future studies will include biochar ecotoxicity analyses and measure carbon–energy balance.
The coffee industry and landfill leachate treatment generate residual waste streams, known as spent coffee grounds (SCG) and landfill leachate membrane concentrate (LLMC). Current practices for managing these residues, including open burning, incineration, and landfilling as a final disposal method, represent a waste of resources and pose a challenge to sustainability. Due to the high pollution potential of solid waste SCG and LLMC, cost-effective management solutions are urgently needed. The present research investigates the slow pyrolysis of SCG using potassium hydroxide (KOH) (weight ratio of 1:1) and LLMC residue (weight ratio of 1:1) as activating agents. The high content of alkali and alkaline earth metals in LLMC could promote the activation of the resulting char and improve the quality of the carbon-based material produced in pyrolysis. The use of LLMC as an activating agent could be a sustainable alternative for valorizing SCG and landfill wastes, potentially replacing ingredients such as steam, CO2, and chemical additives used on an industrial scale. The SCG had a low specific surface area (4.5 m2 g-1), contrasting with the notable surface areas observed in both activated chars. In particular, the KOH-activated char exhibited a higher surface area than the LLMC-activated char, measuring 1,960 m2 g-1 compared to 1,138 m2 g-1 – a difference of about 72%. On the other hand, the combustion enthalpy of the LLMC-activated material was estimated at 22.04 MJ kg-1. The combustion enthalpy of LLMC-activated char was about 21.7% and 19.8% higher than that of SCG and KOH-activated chars, which had values of 18.11 and 18.40 MJ kg-1, respectively. Our findings confirm that pyrolysis of SCG with KOH produces a microporous material with a high specific surface area. In contrast, the resulting LLMC-activated char demonstrates a higher value of combustion enthalpy. This work showed that both activated chars had superior energetic and morphological properties compared to the non-activated char made from SCG biomass. Among the activating agents, KOH led to better performance in terms of char yield and morphological properties. Meanwhile, utilizing LLMC residue as an activating agent highlights its potential for converting landfill waste into high-value material.
1 January 2026 in Engenharia Sanitaria e Ambiental
The coffee industry and landfill leachate treatment produce waste: spent coffee grounds (SCG) and landfill leachate membrane concentrate (LLMC). Current disposal methods, such as open burning, incineration, and landfilling, waste resources and hinder sustainability. Due to their high pollution potential, cost-effective management solutions are urgently needed. This research explores the slow pyrolysis of SCG using potassium hydroxide (KOH) and LLMC as activating agents (1:1 weight ratio). LLMC’s high alkali and alkaline earth metal content may enhance char activation and improve char quality. Using LLMC as an activating agent offers an alternative to value SCG and landfill waste, potentially replacing industrial-scale activators like steam, CO2, and chemical additives. SCG had a low specific surface area (4.5 m2 g-1), contrasting with the notable surface areas observed in both activated chars. In particular, the KOH-activated char exhibited a higher surface area than the LLMC-activated char, measuring 1.960 m2 g-1 compared to 1.138 m2 g-1 - a difference of about 72%. On the other hand, the combustion enthalpy of the LLMC-activated material was estimated at 22.04 MJ kg-1. The combustion enthalpy of LLMC-activated char was about 21.7% and 19.8% higher than that of SCG and KOH-activated chars, which had values of 18.11 and 18.40 MJ kg-1, respectively. This work showed that both activated chars had superior energetic and morphological properties compared to non-activated chars made from SCG biomass. Among the activating agents, KOH led to better performance in terms of char yield and morphological properties. Meanwhile, utilizing LLMC as an activating agent highlights its potential for converting landfill waste into high-value material.