Xiang Li

Mr. Xiang Li

orcid

Research Focus & Metrics

Academic Career Length

2Years (2025-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
25 January 2025 in International Journal of Fatigue
Verified
Journal Article
Closed access
YDYihui Dong
Yihui Dong
DZDongfang Zeng
Dongfang Zeng
HZHai Zhao
Hai Zhao
PWPingbo Wu
Pingbo Wu
YSYe Song
Ye Song
LLLiantao Lu
Liantao Lu

13 December 2025 in Tribology International
Verified
Journal Article
Closed access
DZDongfang Zeng
Dongfang Zeng
YDYihui Dong
Yihui Dong
HZHai Zhao
Hai Zhao
MGMinwei Guan
Minwei Guan
MRMingming Ren
Mingming Ren
LLLiantao Lu
Liantao Lu

15 June 2026 in Metals
Verified
Journal Article
Open access
PDF file
MFMingzhe Fan
Mingzhe Fan
GZguanzhen Zhang
guanzhen Zhang
XLXiang Li
Xiang Li
GLGuang Li
Guang Li
YHYizhu He
Yizhu He
PLpengtao liu
pengtao liu
This study investigated the relationship between the surface microstructure of pearlite steel wheels and the formation of fatigue cracks during the braking process by using a full-size wheel braking test rig. After fatigue failure, the surface microstructural evolution and fatigue crack initiation and propagation of the wheel sample were systematically analyzed by optical microscope (OM), scanning electron microscope (SEM), and transmission electron microscope (TEM). The results showed that after braking of 1572 cycles, a large number of fatigue cracks formed at the wheel tread, which caused the wheel to break. After fatigue failure, some dark areas formed at the wheel tread, which were composed of Fe3O4 compounds. This indicates that severe oxidation was produced at the wheel tread during braking due to the high temperature. After fatigue failure, a continuous thermal white etching layer (T-WEL) was formed in some areas of the wheel tread, while crescent-shaped T-WEL was found in other areas. The microstructure of the T-WEL was composed of martensite phase. The rapid increase and decrease in temperature at the wheel tread during the braking process caused martensitic transformation at the wheel tread. The hardness of the sample reached to about 900 HV in WEL and it reduced with the increase in distance from the surface. The cracks were initiated from the surface and gradually propagated into the matrix. However, the crack propagation mode in the continuous T-WEL and crescent-shaped T-WEL was different. In the continuous T-WEL, the continuous T-WEL of the wheel can be peeled off during the braking wear process, and then the crack was gradually propagated into the matrix in the T-WEL peeled area. As for the crescent-shaped T-WEL, due to the large hardness difference between T-WEL and pearlite, the crack initiated at the interface between the T-WEL and pearlite and gradually propagated into the matrix.

6 July 2026 in Materials
Verified
Journal Article
Open access
PDF file
MFMingzhe Fan
Mingzhe Fan
YFYuming Fu
Yuming Fu
GLGuang Li
Guang Li
XLXiang Li
Xiang Li
SZSa Zhao
Sa Zhao
CZChi Zhang
Chi Zhang
Pearlitic wheel steel subjected to thermal–mechanical fatigue (TMF) during braking can undergo catastrophic fracture. This study clarifies the microstructural evolution governing the macroscopic cyclic hardening/softening behavior of pearlitic wheel steel under thermal–mechanical fatigue (TMF) with a constant mechanical strain range of −0.4% to +0.2%. At lower temperature amplitudes (200–500 °C), the geometrically necessary dislocation (GND) density reaches 20.4 × 1014/m2 during initial cycles, corresponding to cyclic hardening due to dislocation pile-ups at cementite lamellae interfaces. With increasing cycles, the GND density decreases to 12.3 × 1014/m2, concurrent with softening arising from lamellar bending/fracture, partial spheroidization, and dynamic recrystallization of ferrite. At higher temperature amplitudes (200–730 °C), the GND density decreases from 8.8 × 1014/m2 to 3.5 × 1014/m2, reflecting sustained cyclic softening dominated by thermally activated mechanisms, including cementite spheroidization and dislocation annihilation. The resulting softened microstructure consists of ferrite grains, intragranular dispersed cementite, and chain-like coarse cementite at boundaries. Unlike previous studies that focused on single loading conditions (e.g., thermal fatigue, rolling contact fatigue, or wear), the present work addresses the more complex TMF scenario and quantitatively elucidates the interplay between mechanical response and microstructural evolution in pearlitic steel. This work provides theoretical guidance for the development of a fatigue life prediction model for pearlitic wheels under braking.