11 January 2023 in Materials Science and Engineering: A
Verified
Journal Article
Closed access
JZJianyue Zhang
Jianyue Zhang
ECEmre Cinkilic
Emre Cinkilic
XHXuejun Huang
Xuejun Huang
GWGerry Wang
Gerry Wang
YLYuchao (Chad) Liu
Yuchao (Chad) Liu
ALAN LUOALAN LUO
ALAN LUO

4 February 2022 in Journal of Magnesium and Alloys
Verified
Journal Article
Open access
YFY. Fu
Y. Fu
GWGerry Wang
Gerry Wang
AHA. Hu
A. Hu
YLY. Li
Y. Li
KTK.B. Thacker
K.B. Thacker
HHHenry Hu
Henry Hu
Sludge consisting of heavy element phases and oxides is often generated during the casting operation of aluminum (Al) and magnesium (Mg) alloys. With the help of the well-established Sludge Factor (SF) formula, it is relatively easy to control the sludge generation in aluminum alloys. But formation mechanisms and characteristics of sludge in die casting magnesium alloys are still unclear. To ensure the production of high quality die cast components at a low cost, a full understanding of sludge in die casting Mg alloys and its proper control measures need to be developed, since excessive sludge formation affects deleteriously material and operation cost, and casting performance. In the present report, the formation, characteristics and control of Mg die-casting sludge, based on the established knowledge of sludge formation and sludge factor in Al die casting alloys, are reviewed. Previous work on characterization and assessment of sludge in die cast Mg alloys are reviewed. Metallurgical principles for control of sludge in ingot production in association with die casting of Mg alloys are discussed. Rapid assessment of Mg oxide and intermetallics relevant to sludge formation in Mg alloys are highlighted.

1 June 2018 in Journal of Magnesium and Alloys
Verified
Journal Article
Open access
GWGerry Wang
Gerry Wang
JBJeremy Bos
Jeremy Bos
With tremendous weight saving potential, magnesium alloy high pressure die casting components have been widely used for automotive applications. Magnesium fastening technology is thus becoming increasingly important to design engineers. Joining as-cast holes of magnesium high pressure die casting components with thread forming fasteners provides significant advantages for the assembly process, overall cost benefit and joint integrity. This type of joint is thus preferred for structural applications. Designing the thread forming fasteners with as-cast holes follows the general rules for designing for the machined holes, including carefully designing the variables such as the assembly torque range, the length of thread engagement, the hole diameter and required failure mode. In addition, special attention needs to be paid to the draft angles of the magnesium cast components that are required for the die casting process. In this paper, the effects of above key factors, individually and combined, on the joint performance of thread forming fasteners with as-cast blind holes of AM60B magnesium components are studied. A joint design philosophy was proposed to optimize both joint performance (the prevailing torque, the failure torque and the failure mode) and manufacturing easiness (the hole diameter and corresponding draft angle). The detailed design considerations for as-cast holes of magnesium HPDC are discussed and explained through a hypothetical example.

11 August 2020 in SAE International Journal of Materials and Manufacturing
Verified
Journal Article
Closed access
GWGerry Wang
Gerry Wang
KMK. MacKenzie
K. MacKenzie
CSC. Sweet
C. Sweet
JCJ.T. Carter
J.T. Carter
JOJ.C. O’kAne
J.C. O’kAne
ALAN LUOALAN LUO
ALAN LUO
Cast magnesium (Mg) door inner panels can provide a good combination of weight, functional, manufacturing, and economical requirements. However, several challenges exist including casting technology for thin-wall part design, multi-material incompatibility, and relatively low strength versus steel. A project was supported by the US Department of Energy to design and develop a lightweight frame-under-glass door having a thin-wall, full die-cast, Mg inner panel. This development project is the first of its kind within North America. The 2.0 mm Mg design, through casting process enablers, has satisfactorily met all stiffness and side-impact requirements, with significant mass reduction and part consolidation. In addition, a corrosion mitigation strategy has been established using industry-accepted galvanic isolation methods and coating technologies. The performance of the Mg design has been demonstrated through component and vehicle tests. This article is an updated publication of a previously published International Mg Association (IMA) proceedings paper [1] (with agreement from the Association).


21 April 2024 in Journal of Magnesium and Alloys
Verified
Journal Article
Open access
YFY. Fu
Y. Fu
GWGerry Wang
Gerry Wang
AHA. Hu
A. Hu
YLY. Li
Y. Li
KTK.B. Thacker
K.B. Thacker
HHHenry Hu
Henry Hu
Intermetallic formation in sludge during magnesium (Mg) melting, holding and high pressure die casting practices is a very important issue. But, very often it is overlooked by academia, original equipment manufacturers (OEM), metal ingot producers and even die casters. The aim of this study was to minimize the intermetallic formation in Mg sludge via the optimization of the chemistry and process parameters. The Al8Mn5 intermetallic particles were identified by the microstructure analysis based on the Al and Mn ratio. The design of experiment (DOE) technique, Taguchi method, was employed to minimize the intermetallic formation in the sludge of Mg alloys with various chemical compositions of Al, Mn, Fe, and different process parameters, holding temperature and holding time. The sludge yield (SY) and intermetallic size (IS) was selected as two responses. The optimum combination of the levels in terms of minimizing the intermetallic formation were 9 wt.% Al, 0.15 wt.%Mn, 0.001 wt.% (10 ppm) Fe, 690 °C for the holding temperature and holding at 30 mins for the holding time, respectively. The best combination for smallest intermetallic size were 9 wt.% Al, 0.15 wt.%Mn, 0.001 wt.% (10 ppm) Fe, 630 °C for the holding temperature and holding at 60 mins for the holding time, respectively. Three groups of sludge factors, Chemical Sludge (CSF), Physical Sludge (PSF) and Comprehensive Sludge Factors (and CPSF) were established for prediction of sludge yields and intermetallic sizes in Al-containing Mg alloys. The CPSF with five independent variables including both chemical elements and process parameters gave high accuracy in prediction, as the prediction of the PSF with only the two processing parameters of the melt holding temperature and time showed a relatively large deviation from the experimental data. The Chemical Sludge Factor was primarily designed for small ingot producers and die casters with a limited melting and holding capacity, of which process parameters could be fixed easily. The Physical Sludge Factor could be used for mass production with a single type of Mg alloy, in which the chemistry fluctuation might be negligible. In large Mg casting suppliers with multiple melting and holding furnaces and a number of Mg alloys in production, the Comprehensive Sludge Factor should be implemented to diminish the sludge formation.