This study develops a kinetic model that captures poly-ether-ether-ketone (PEEK) crystallization over a temperature window from glass transition () to melting () temperature, and across cooling rates from 5 to ~103 °C/min. The framework is a parallel dual-Nakamura formulation whose isokinetic parameters {} are obtained from a bi-level non-linear regression of isothermal crystallization tests conducted using a flash-differential scanning calorimeter (FSC). The weight partitions the faster primary and slower secondary crystallization and is represented by a physics-based analytical function that captures its dome-shaped temperature dependence. A maximum isothermally achievable enthalpy function is introduced so that the model predicts enthalpy natively under arbitrary thermal profiles. To extend this isothermal backbone to non-isothermal conditions, two explicit cooling-rate-dependent scalars are introduced, and , which shift and limit attainable crystallinity at high cooling rates respectively. Finally, a rate-dependent induction time relation is added to adjust the onset of crystallization. Calibrating these rate functions against non-isothermal experiments, while keeping the isokinetic parameters fixed, yields a single isothermal–non-isothermal model that predicts under arbitrary profiles. Model performance is validated using an interrupted FSC experiment with a multi-segment cooling program that mimics a local transient thermal history of PEEK during additive manufacturing. The sample is cooled through successive constant-rate segments with intermittent quench–remelt cycles to probe the accumulated crystallinity along the path. Without additional fitting, the model predicts the measured enthalpy evolution with R2 ≈ 0.95. The framework thus provides a practical route for predicting polymer crystallinity under processing-relevant thermal histories.
17 March 2026 in Advanced Composites and Hybrid Materials
In this study, we developed UV-laser-induced carbon nanosphere/graphene (UV-LICNG) composites using a single-step ablation technique. This method employs UV-laser-induced forward transfer (UV-LIFT) to directly fabricate line-patterned UV-LICNG composites on silane-terminated polyurethane (S-PU) substrates with excellent mechanical properties. The unique structure of UV-LICNG, comprising conjugated carbon nanospheres and graphene with a large surface area, enables outstanding strain and humidity sensing performance. Owing to a separation-based sensing mechanism, the UV-LICNG-based strain sensor exhibits highly sensitive strain detection in the low-strain regime, achieving a high gauge factor (GF ≈ 146.5 within the 0–2% strain range), along with excellent linearity (R² ≈ 0.9906), rapid response and recovery times (29 ms and 31 ms, respectively), and exceptional durability over 3,000 stretching cycles at 0.2% strain. These attributes enable precise detection of subtle human motions and vocalization-induced strain signals. In addition, the intrinsic nano–micro porous graphitic structure of UV-LICNG imparts excellent humidity-sensing performance, characterized by fast response and recovery times (4.2 and 4.8 s, respectively), thereby facilitating reliable respiration monitoring and non-contact skin humidity sensing. The combined strain and humidity sensing capabilities, together with the simplicity and scalability of the UV-LIFT process, highlight the strong potential of UV-LICNG-based wearable electronics for continuous human health monitoring and multifunctional wearable sensing applications.
A flexible skin patch based on thermochromic liquid crystals (TLCs) embedded within a polydimethylsiloxane (PDMS) elastomer is presented for passive visualization of skin–vein thermal contrasts. Five ternary TLC formulations composed of cholesteryl oleyl carbonate (COC), cholesteryl nonanoate (CN), and cholesteryl benzoate (CB) were systematically engineered to tune mesophase stability and helical pitch sensitivity within the physiological temperature range (32–37 °C). Small compositional adjustments (≤1 wt.%) produced pronounced and predictable shifts in color-play bandwidth and optical sensitivity, governed by thermally induced contraction of the cholesteric helix. Patterned TLC microdomains were integrated onto optically absorptive PDMS substrates and encapsulated within a transparent PDMS overlayer, yielding thin, mechanically compliant, and breathable films with uniform thermal transmission. Optical spectroscopy, optical microscopy, and RGB analysis revealed linear wavelength–temperature relationships (R2 > 0.9) and red-to-green sensitivities of up to ~87 nm °C−1, demonstrating high thermochromic sensitivity within the physiological skin temperature range. Mechanical characterization confirmed skin-matched elasticity, while preliminary sterilization studies indicated that the films retained their mechanical properties following ethanol immersion and UV exposure. As a feasibility study, the results demonstrate the potential of a compositionally tunable thermochromic elastomer platform for visualizing physiological skin temperature variations associated with superficial veins, providing a basis for further development toward wearable vein visualization for self-cannulation in home hemodialysis and related thermal sensing applications.