As a skeleton material, polyester (PET) fiber can significantly improve the strength and durability of rubber composites, but the interfacial adhesion between polyester fiber and rubber is poor due to the chemical inertia of PET fiber surface. Resorcinol-formaldehyde-latex (RFL) impregnating solution is usually used to treat PET fibers, but RFL contains toxic components such as resorcinol, which is harmful to the human body. A simple and less toxic resin-impregnating system cresol-formaldehyde-latex (CFL) was obtained by alternating resorcinol with low-toxicity cresol and m-cresol formaldehyde resin was synthesized from m-cresol and formaldehyde. CFL (m-cresol formaldehyde resin latex) systems with different C/F mole ratios and CF resin/latex ratios were adopted to modify the surface of PET fibers. The strip peeling adhesive and the H pull-out test results indicated that the PET fiber/rubber adhesion strength increased with the increase in the formaldehyde dosage and the CF resin content, and the peeling force value and the H-pull-out force of treated PET/rubber composites reached 7.3 N/piece and 56.8 N, respectively. The optimal choice of CFL adhesive system was obtained, when the C/F mole ratio was 1/2 and the CF resin/latex weight ratio was 0.23. This environment-friendly CFL dipping emulsion can be used as a new surface modification strategy as it can remarkably enhance the interfacial adhesion of PET/rubber composites.
Electromagnetic interference (EMI) shielding materials are critical for reducing EMI pollution and enhancing information security. This study presents a systematic comparison of silver-plated copper (Cu@Ag; flake-like morphology; the average particle size D50 = 20.1 μm) and silver-plated aluminium (Al@Ag; spherical morphology; D50 = 47.5 μm) fillers with distinct morphologies incorporated into silicone rubber matrices via Rheomixer blending, open-mill compounding, and peroxide vulcanisation. This work aims to elucidate how filler morphology and multilayer sandwich architecture govern shielding efficiency and related material properties. The flake-like Cu@Ag fillers demonstrated superior low-loading performance. Due to their high aspect ratio and enhanced interfacial contact, Cu@Ag composites reached a critical loading for practical EMI shielding performance at 150 phr. In contrast, spherical Al@Ag fillers required a higher loading of 200 phr to achieve the same effect. Both composites achieved EMI shielding effectiveness exceeding 90 dB at 250 phr filler loading across the X-band frequency range (8.2–12.4 GHz). Innovatively, sandwich-structured composites were fabricated by combining Cu@Ag and Al@Ag layers through co-vulcanization, achieving approximately 110 dB shielding effectiveness, which is a ~33% improvement over single-layer composites at equivalent filler loading (200 phr). Analysis of the shielding mechanisms reveals that this enhancement results from multiple electromagnetic wave interactions, including increased reflection losses at morphologically distinct layer interfaces and enhanced absorption through conductivity gradients. This work demonstrates that a rational combination of flake-like and spherical fillers with contrasting morphologies and conductivity characteristics in multilayer architectures provides a powerful strategy for developing high-performance flexible EMI shielding materials.