The creep behavior at an ambient temperature of typical h.c.p., b.c.c. and f.c.c. metals and alloys of annealed states were surveyed. Cubic metals and alloys demonstrated negligible creep strain under all stress ranges. In contrast, h.c.p. metals and alloys demonstrated significant creep behavior. In particular, Ti–6Al–4V alloy and CP–Ti metal showed accumulated large creep strains. The difference among metals and alloys were negligible, for Mg and Zr. After being cold rolled, Ti–6Al–4V alloy and CP–Ti metal showed less significant creep behavior.
15 June 2009 in Materials Science and Engineering: A
The high-temperature deformation process of the recrystallized 16CrODS ferritic steel was investigated at 1000°C for the stress loading perpendicular to the elongated grain structure. The strain rate was varied in the range from 1.0×10−2 to 1.0×10−5s−1. At the strain rate over 1.0×10−4s−1, deformation is dominated by the conventional dislocation creep. Decreasing strain rate from 1.0×10−4s−1, grain boundary sliding becomes prominent. Accommodation process for the localized stress induced by grain boundary sliding could be dislocation creep at 1.0×10−4s−1, and by diffusional creep at 1.0×10−5s−1 or less. These were verified through the observation of void formation and localized strain accumulation by KAM map