Ali Alizadeh

Dr. Ali Alizadeh


Research Focus & Metrics

Academic Career Length

9Years (2018-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 January 2021 in Transactions of Nonferrous Metals Society of China
Verified
Journal Article
Open access
MSMatin Saessi
Matin Saessi
AAAli Alizadeh
Ali Alizadeh
AAAlireza Abdollahi
Alireza Abdollahi
Tribological behavior and wear mechanisms of mechanically milled Al5083 alloy and Al5083−5wt.%B4C composite at room temperature and 200 °C were discussed. Results revealed that due to the oxidative wear at room temperature, a mechanically mixed layer (MML) was formed to protect the surface of the samples. Under 80 N of load at room temperature, the milled Al5083 and the Al5083−5wt.%B4C samples showed evidence of abrasion with limited volume loss. In this case, the wear rates were 5.8×10−7 and 4.4×10−7 mm3/(m·N), respectively. At 200 °C and under 80 N of applied load, severe wear occurred in the milled Al5083 sample, and wear rate reached 10.8×10−7 mm3/(m·N) while the Al5083−5wt.%B4C sample showed mild wear with local 3-body abrasion and the wear rate reached 5.3×10−7 mm3/(m·N). Strengthening mechanisms such as dislocation pinning and the Hall−Petch theory, high hardness and the load transfer effect were crucial in determining the wear behavior of the Al5083−5wt.%B4C composite. On the other hand, the milled Al5083 sample represented a relatively high wear rate at 200 °C, which seemed to be related to the local grain growth and a drop in its hardness.

20 December 2018 in Materials Research Express
Verified
Journal Article
Closed access
PDF file
AAAli Alizadeh
Ali Alizadeh
MGMaryam Geraei
Maryam Geraei
MMMohammad Reza Mahoodi
Mohammad Reza Mahoodi
In this study, the fabrication of Al-Al2O3-TiB2 hybrid composite using TiO2, B2O3, and Al5083 powders through aluminothermy method has been studied. TiO2, B2O3, and Al5083 powders were attrition milled (20:1 bullet to powder ratio, under argon atmosphere, the speed of 650 rpm for 2, 4, 6 and 20 hours). After the completion of the milling process, the milled powder was added to the aluminum molten at 900°C and finally, the Al5083-Al2O3-TiB2 composite was produced in situ. After the hot extrusion process, specimens were characterized by SEM and XRD analyses and the strength of the composite was investigated. The results of the microstructure analysis and the strength of the specimens indicate the efficiency of low milling times and the absence of TiB2 in milling. The observations from microstructure show presence of TiB2 ceramic particles less than 300 nm in size. The strength tests done on 2, 4, 6 and 20-hour specimens represent values of 294, 336, 295 and 276 MPa, respectively.

1 January 2019 in Transactions of the Indian Institute of Metals
Verified
Journal Article
Closed access
PDF file
AAAli Alizadeh
Ali Alizadeh
MBMohammad Hossein Babaee
Mohammad Hossein Babaee

6 October 2021 in Transactions of the Indian Institute of Metals
Verified
Journal Article
Closed access
PDF file
AAAli Alizadeh
Ali Alizadeh
AAAlireza Abdollahi
Alireza Abdollahi
MSMatin Saessi
Matin Saessi