In this study, deposition of a Ni3P nano-scale layer on B4C nanoparticles via simple electroless plating in an acidic bath was investigated. B4C nanoparticles were produced by mechanical milling with the average size of about 95 nm. Electroless nickel plating was carried out at temperature and pH of 85°C and 5.5, respectively. The uncoated and composite powders were characterized by transition electron microscope and the phases present were revealed by X-ray diffraction. Also, nickel and phosphorous contents of the coating were measured by inductively coupled plasma analysis. The results confirmed deposition of a Ni3P layer with the average thickness of about 25 nm on B4C nanoparticles.
28 September 2017 in International Journal of Materials Research
The microstructure and mechanical properties of Al–Zn–Mg/3 wt.% Al2O3 composite were modified through a thermomechanical processing technique. The powders were cold pressed and solid state sintered for 90 min under argon atmosphere. Thermomechanical processing was then applied to the solid state sintered samples, which consisted of cold pressing followed by partial remelting for 30 min under argon atmosphere. Four different loads in the thermomechanical processing were used to investigate the effects of compressive loads on the microstructures and the mechanical properties. The results revealed modifications in the microstructure of the thermomechanically processed samples with the optimum combination of properties in the sample modified by applying the load of 250 MPa. Increasing the thermomechanical processing load decreased the amounts of porosity by about 7 %, decreased the average grain size to about 4 μm, enhanced the compressive yield strength to about 295 MPa, and increased the microhardness values from 250 HV to 600 HV. In addition, the energy absorption capacity increased by about three times.
4 January 2016 in Acta Metallurgica Sinica (English Letters)