In order to decrease CO2 emission from the ironmaking process, an increasing use of hydrogen in blast furnace (BF) ironmaking is a promising way. In this case, the properties of iron ore sinter such as reducibility and strength need to be optimized because hydrogen reduction of iron oxide is an endothermic reaction and temperature distribution in BF drastically changes. In this study, the effect of hydrogen concentration in the reducing gas on the changes in mineral phases during reduction of iron ore sinter is evaluated. Mineral composition of the ten types of sinter samples was analyzed by XRD and image analysis. Sinter sample was reduced under the simulated conditions such as Low-H2 (N2 - 48%(CO + CO2) - 5.8%(H2 + H2O)) and High-H2 (N2 - 48%(CO + CO2) - 13%(H2 + H2O)). After reduction, microstructure of the sample was observed. Iron ore sinters usually consist of mineral phases such as hematite, magnetite, calcium-ferrites and slag. Furthermore, calcium-ferrite phases are roughly divided into four types: 1) acicular texture coexisted with primary hematite (1H-ACF), 2) columnar texture coexisted with secondary hematite (2H-CF), 3) small and 4) large columnar textures coexisted with magnetite (M-FCF and M-CCF). An increase in hydrogen concentration of reducing gas accelerates the reduction of hematite, 1H-ACF, and 2H-CF in all sinter samples, while it does not affect the reduction of magnetite, and calcium-ferrite coexisted with magnetite.
Currently, the Japanese steel industry is developing the technologies to reduce 30% of domestic CO₂ emissions from iron- and steelmaking industry using an innovative ironmaking process such as the COURSE50 project, which focuses on H2 reduction and CCUS technologies. On the other hand, it has been reported that an increasing H2 gas ratio in the blast furnace reducing gas promotes the low temperature reduction disintegration of the iron ore pellet. In this study, the low temperature reduction disintegration mechanism of self-fluxing pellet under higher hydrogen condition at 500°C was examined. During hydrogen reduction which proceeds uniformly, the fine cracks with few micrometers in the primary particles form. It leads to the formation of fine particles with the size of less than 0.1 mm on the surface of the pellet. Increase in the particles with few millimeters makes a significant impact on the permeability of the blast furnace. On the other hand, CO reduction without hydrogen gas proceeds topochemically, and volumetric fracture progresses with generation of the cracks with several millimeters in length due to the stress difference between near the surface and in the center of pellet. Under higher H2 conditions, reduction proceeds uniformly, so such cracks causing volume fractures are hard to form, but the finer cracks are easier formed than the case of CO reduction, and the amounts of finer particles increases.
For decreasing carbon dioxide emission from iron- and steelmaking industry, hydrogen utilization in the blast furnace has been considered. Iron ore sinter is one of the major iron sources for the blast furnace. It is known that the effects of the hydrogen concentration in the reducing gas on the reducibility and reduction disintegration of the sinter are strong. In this study, the evaluation of the mineral phase of the Mosaic EmBedding Iron Ore Sintering (MEBIOS) sinter and reducibility using a laboratory scale furnace simulated the blast furnace condition with high hydrogen concentration and the experimental blast furnace were carried out.MEBIOS sinter has higher ratio of the mineral phases, i.e., hematite and acicular calcium ferrite with primary hematite, showing higher reducibility compared to the conventional sinters. The value of JIS-RDI of the MEBIOS sinter decreases with an increase in that of JIS-RI, which is the reverse trend of the conventional sinter. Further, the basket charge test with the experimental blast furnace confirmed that the MEBIOS sinter shows high reducibility under the condition of high hydrogen concentration while the reduction disintegration behavior at low temperature is similar to conventional sinter.
It has been reported that an increasing H2 gas ratio of the reducing gas in the blast furnace promotes the low temperature reduction disintegration of the iron ore pellet. Reduction of the pellet sample proceeds uniformly under higher H2 condition at 500°C. Microcracks with the size of several micrometer form at the primary particles of iron oxide and it promote fine particles formation after the drum test. Macrocracks with the size of several millimeter form inside of the pellet after reduction and it promotes the volumetric destruction. In this study, the temperature dependence of reduction disintegration of self-fluxing pellet under higher H2 condition was examined.Pellet sample was reduced under CO and CO-H2 gas conditions at 600°C and 700°C. After reduction, the disintegration test was conducted using the drum. Under higher H2 condition at 600°C, the density of microcracks decreases with increasing reduction degree and it leads to lower of the RDI value than that at 500°C. The reason is that the volumetric expansion by the reduction from hematite to magnetite at 600°C is not significant compared with that at 500°C. The difference of reduction degree at the center and near the surface of the pellet increases with increasing the reduction temperature. Reduction reaction proceeds more topochemically by increasing reduction temperature and the addition of hydrogen. This change leads the macrocrack formation, which is same mechanism under CO gas condition at 500°C. At 700°C, on the other hand, this microcrack was not observed because the volumetric expansion by the reduction is lower than that at lower temperature. Therefore, the effect of hydrogen addition on disintegration is not significant at 700°C.