A flexible polyimide-based single-walled carbon nanotube (SWCNT) thermal film sensor has been developed for wall shear stress measurements in both air and water. To ensure high sensitivity, vacuum thermal annealing and electrical aging are conducted to enhance the electric properties of the sensor with low-resistance and the high temperature coefficient of resistivity (TCR). The TCR of sensors can reach to 8040 ppm/°C to the author’s knowledge, which is the highest reported value of thermal sensors used for shear stress measurements. In calibration, the output voltage of the sensor is proportional to the one third power of wall shear stress with the sensitivity on the order of mV Pa −1 in the constant current operation mode. The repeatability error is no more than 1% in both air and water, which confirms the capability of the flexible SWCNT thermal film sensor for fluid wall shear stress measurements with high sensitivity.
Wall fluctuating pressure in the boundary layer is critical for physical understanding of the surface flow and detection resolution optimization of the underwater vehicle. In this study, a flexible MEMS vanadium-doped zinc oxide (VZO) film piezoelectric pressure sensor array is developed for underwater applications. 2% vanadium-doped zinc oxide film achieves figure of merit of -54.5, far higher than the previous records of the contemporary thin films, indicating excellent receiving sensitivity. The sensors are designed and fabricated using a 4-mask VZO-on-SOI process. An array of 2×5 sensors is flexibly integrated on a polyimide foil and insulated by a parylene C waterproof cover. Calibrations in a plane wave tube are demonstrated. About 0.64± 0.06 mV/Pa pressure sensitivity at the frequency of 10 Hz to 2 kHz and the maximum nonlinearity of 0.3% from 0 to 50 Pa are achieved. The capabilities of the flexible sensors array in a real-time sensing situation on an underwater vehicle model are validated. The laminar, transition and turbulent flow at different positions of the vehicle model are detected successfully from the sensor outputs. The result shows that the amplitude and power energy of the fluctuation pressure at the transition case are higher than that of the laminar and turbulent flow. The presented sensors array with merits of low power, miniature size and low foot-print, offers a flexible and readily surface-mountable system, exhibiting promising potentials in underwater applications.
A high-performance micromachined piezoelectric sensor based nanostructured vanadium-doped zinc oxide (ZnO) film with air-backing has been developed and characterized for underwater acoustic application. The sensing cell with a low foot-print of 2.0 mm × 2.0 mm is fabricated by Micro electro mechanical systems (MEMS) technology using a ZnO-on-silicon-on-insulator process platform. An optimal ratio of piezoelectric coefficient to the relative permittivity is obtained about 6.3 in the Zn 0.98 V 0.02 O sensing cell, improving by an order of magnitude compared with other notable piezoelectric films, plays a mainly dominant role in the enhanced piezoelectric response. Calibrations in the standard underwater instrument have demonstrated that the presented sensor could achieve an acoustic pressure sensitivity of −165 ± 2 dB (1 V μ Pa −1 ) over a bandwidth 10 Hz–10 kHz, outperforming the same kind of reported devices. The maximum non-linearity is no more than 0.3%, the sensitivity variation is no more than ±0.7 dB in the temperature range from 10 °C to 50 °C, indicating a better stability and higher reliability. The proposed sensor with a superior acoustic sensitivity gives a great application potential in underwater acoustic measurements.
The development of multi-role flexible thermal films embedded with single-walled carbon nanotubes (SWCNTs) exhibiting an adjustable temperature coefficient of resistance (TCR) is presented. The composite film is prepared by an alternating electric field to assembling CNTs on Ni conductive layer and polyimide. Modified vacuum thermal treatment is then conducted to adjust the TCR behavior of films, thereby gaining the positive, negative and near-zero TCR ranging from −1.5% °C −1 to nearly 1.0% °C −1 at different annealing conditions, respectively. The changes of morphologies, tube crystallinity and chemical elements in films are investigated. The enhanced intertube couplings in bundles of CNTs, formations of chemical bonds and recrystallization in heat-treated films, resulting in the change of charge transport, play a dominant role in the evolution of the TCR behavior. Heat-treated films also exhibit linear temperature dependence and high stability while operating at wide ambient temperature, leading to broad prospects in flexible electronic thermal applications.