Thermal abuse of lithium-ion batteries (LIBs) leads to the emission of gases, solids, fires and/or explosions. Therefore, it is essential to define the temperatures at which key events occur (i.e., CID activation, venting, and thermal runaway (TR)) and to identify the related emissions for identifying the hazards to which people and especially rescue teams are exposed. For this purpose, thermal abuse tests were performed on commercial lithium nickel cobalt aluminum oxide (NCA) 18650 cells at 50% state of charge in a reactor connected to an FT-IR spectrometer by varying test conditions (feed gas of N2 or air; heating rates of 5 or 10 °C/min until 300 °C). In particular, the concentrations of the gases and the composition of the condensed-phase emissions were estimated. As regards gases, a high concentration (1695 ppmv) of hydrofluoric acid (HF) was measured, while the emissions of condensed matter consisted of organic compounds such as polyethylene oxide and paraffin oil, and inorganic compounds containing Li (0.173 mg/m3) and Al (0.344 mg/m3). The main safety concerns were caused by the temperatures (564 ± 85 °C) reached by the cell during TR, by the HF concentration which exceeded the toxicity limits of 30 ppm, the IDLH defined by the NIOSH, and the diameter of the particles (1.54 ± 0.69 µm) that rose the PM2.5 concentration. These results are also useful for identifying personal protection equipment for rescue teams.
20 June 2024 in Case Studies in Chemical and Environmental Engineering
Lithium-ion batteries (LIBs) are employed when high energy and power density are required. However, under electrical, mechanical, or thermal abuse conditions a thermal runaway can occur resulting in an uncontrollable increase in pressure and temperature that can lead to fire and/or explosion, and projection of fragments. In this work, the behavior of LIBs under thermal abuse conditions is analyzed. To this purpose, tests on NCA 18,650 cells are performed in a cone calorimeter by changing the radiative heat flux of the conical heater and the State of Charge (SoC) of the cells from full charge to deep discharge. The dependence of SoC and radiative heat flux on the thermal runaway onset is clearly revealed. In particular, a deep discharge determines an earlier thermal runaway of the cell with respect to those at 50% and 100% of SoC when exposed to high radiative heat flux (50 kW/m2). This is due to a mechanism such as an electrical abuse. Cell components before and after tests are investigated using Differential Scanning Calorimetry (DSC), Scanning Electron Microscopy—Energy Dispersive X-ray Spectroscopy (SEM-EDS) and X-ray Diffraction (XRD) to determine the structural, morphological, and compositional changes. It results that the first reaction (423–443 K) that occurs at the anode involves the decomposition of the electrolyte. This reaction justifies the observed earlier venting and thermal runaway of fully charged cells with respect to half-charged ones due to a greater availability of lithium which allows a faster kinetics of the reaction. In the cathode residues, metallic nickel and NO are found, given by decomposition of metal oxide by the rock-salt phase cathode.
Lithium-ion batteries (LIBs) are employed in a range of devices due to their high energy and power density. However, the increased power density of LIBs raises concerns regarding their safety when subjected to external abuse. The thermal behavior is influenced by a number of factors, i.e., the state of charge (SoC), the cell chemistry and the abuse conditions. In this study, three distinct cylindrical Li-ion cells, i.e., lithium nickel cobalt aluminum oxide (NCA), lithium titanate oxide (LTO), and lithium iron phosphate (LFP), were subjected to thermal abuse (heating rate of 5 °C/min) in an air flow reactor, with 100% SoC. Venting and thermal runaway (TR) were recorded in terms of temperature and pressure, while the emitted products (gas, solid, and liquid) were subjected to analysis by FT-IR and ICP-OES. The concentrations of the toxic gases (HF, CO) are significantly in excess of the Immediate Danger to Life or Health Limit (IDLH). Furthermore, it is observed that the solid particles are the result of electrode degradation (metallic nature), whereas the liquid aerosol is derived from the electrolyte solvent. It is therefore evident that in the event of a LIB fire, in order to enhance the safety of the emergency responders, it is necessary to use appropriate personal protective equipment (PPE) in order to minimize exposure to toxic substances, i.e., particles and aerosol.
23 December 2025 in Journal of Sustainable Cement-Based Materials