Cementite morphology is known to govern the mechanical performance of steels, yet its influence on actual crystal structure, like unit cell parameters, is not well quantified. Here, we show that cementite morphology-dependent surface stresses generate measurable lattice distortion in nanocrystalline cementite. Lamellar and spheroidized cementite powders were extracted from a Cr-alloyed hypereutectoid steel and characterized by high-energy synchrotron X-ray diffraction combined with double-Voigt profile modeling. Despite a higher Cr content in spheroidized cementite, lamellar cementite exhibits systematically larger lattice parameters, corresponding to an average volumetric lattice strain of 6.3 ± 2.2 × 10−4. This counter-intuitive expansion is rationalized by a continuum mechanics framework that incorporates the orthorhombic elastic anisotropy of cementite and particle morphology. The model predicts the sign and magnitude of morphology-induced lattice strain, demonstrating that surface-stress effects constitute a systematic bias in diffraction-derived lattice parameters of nanostructured carbides.
12 August 2026 in Metallurgical and Materials Transactions A
Cementite spheroidization heat treatments of hypereutectoid steels are of major industrial relevance as a prerequisite for the production of rolling bearing components such as bearing balls, rollers, and races. Owing to their long process durations and high energy demand, optimizing these heat treatments offers significant potential for reducing energy consumption and associated CO 2 emissions. In this work, two fundamentally different cementite spheroidization mechanisms—sub- $$A_{\text {c1}}$$ spheroidization and spheroidization via the divorced eutectoid transformation—are systematically investigated with respect to their microstructural evolution, mechanical properties, and potential for process optimization. This study combines dilatometry, hardness testing, scanning electron microscopy with AI-assisted particle analysis, electron backscatter diffraction, and transmission electron microscopy to establish quantitative correlations between processing parameters, microstructure, and properties. Spheroidization via the divorced eutectoid transformation proves to be superior to sub- $$A_{\text {c1}}$$ heat treatments in terms of time efficiency and achievable spheroidization degree. A broad parameter study covering austenitization temperatures and cooling rates reveals that temperatures slightly above $$A_{\text {c1}}$$ combined with cooling rates of $$125\,^{\circ }\text {C\,h}^{-1}$$ or lower yield the highest spheroidization degrees and the lowest hardness values.