This work introduces a thin-walled, modular flexible structure, the Highly Deformable Structure (HDS), specifically engineered to exhibit bending-dominated behavior and a deployable mechanism, enabling large deformations, high energy absorption, and superior flexibility. HDS specimens were fabricated through Laser Powder Bed Fusion (LPBF) process using three different materials: SS316L, AlSi10Mg and NiTi. The study combined morphological analyses and mechanical characterizations to provide a comprehensive assessment of their performance. The results demonstrate that the HDS geometry accommodates significant deformations without structural failure, confirming the robustness of the design. Dynamic analyses conducted at 2 Hz showed that, among the tested alloys, NiTi exhibited the highest damping capacity, with a tanδ of 0.035 at 1% deformation amplitude, at a mean force of 20 N and at 5 °C (corresponding to austenite start temperature As ). In comparison, SS316L and AlSi10Mg HDS cells also showed excellent dynamic response within the plastic regime at strain below 0.5%. Furthermore, the NiTi-based HDS benefits from shape memory effect, recovering over 50% of the applied deformation, which makes it particularly suitable for impact-resistance applications. These findings highlight the potential of LPBF in developing next-generation metallic components with tunable deformability, enabling advances in load bearing, damping and energy absorbing systems.
Among the ferromagnetic shape memory alloys (SMAs), Ni43Mn31Ga19Co7 (at%) alloys are well known as a promising ferromagnetic SMA (FeSMA) for magnetocaloric effect, and scientific interest has increased due to the possible exploitation of multicaloric function. This first example of multi-effect by coupling elastocaloric and magnetocaloric effect is still far from complete experimental validation, mainly due to the difficulty of testing conditions that require the simultaneous application of both fields. In this study, a low magnetic field (μ0H = 0.26 T and 0.56 T) is applied during elastocaloric deformation at different temperatures. Although the magnetic field values applied in this work are much lower than those usually considered in the magnetocaloric effect, the magnetic field improves the elastocaloric effect, increasing the total strain and reducing the critical stress and mechanical hysteresis. This synergic action allows us to obtain an increase in the ΔTad of about 13% and 25% upon loading and unloading, respectively.