Cellulose extractions from wheat straw via hydrochloric, nitric, and sulfuric acid hydrolysis methods were carried out. X-ray diffraction spectral analyses reveal that depending on the acid conditions used the structure of the cellulose exhibited a mixture of polymorphs (i.e., CI and CIII cellulose phases). In addition, the percent crystallinity, diameter, and length of the cellulose fibers varied tremendously as determined by X-ray diffraction and scanning electron microscopy. Thermal gravimetric analysis measurements revealed that the thermal stability of the extracted cellulose varied as a function of the acid strength and conditions used. Scanning electron microscopy analysis revealed that the aggregation of cellulose fibers during the drying process is strongly dependent upon the drying process and strength of the acids used.
1 January 2015 in International Journal of Polymer Science
The nonuniform distribution of cellulose into many composite materials is attributed to the hydrogen bonding observed by the three hydroxyl groups located on each glucose monomer. As an alternative, chemical functionalization is performed to disrupt the strong hydrogen bonding behavior without significant altering of the chemical structure or lowering of the thermal stability. In this report, we use wheat straw as the biomass source for the extraction of cellulose and, subsequently, chemical modification via the Albright-Goldman and Jones oxidation reactions. X-ray diffraction analyses reveal that upon oxidation a slight change in the cellulose polymorphic structure (CI to CII) can be observed when compared to its unmodified counterpart. Scanning electron microscopy analyses show that the oxidized cellulose structure exhibits fiber-like crystals with lengths and diameters on the micrometer scale. Thermal analyses (differential scanning calorimetry and thermogravimetric analysis) show an increase in the thermal stability for the modified cellulose at extremely high temperatures (>300°C).
Microcrystalline cellulose was explored as possible biodegradable fillers in the fabrication of ABS plastic composites. TGA indicates that upon inclusion of cellulose microcrystals the thermal stability of the ABS plastics was improved significantly when compared to the neat ABS plastic counterparts. Furthermore, inclusion of extracted cellulose from plant biomass showed a higher thermal stability with maximum decomposition temperatures around 131.95°C and 124.19°C for cellulose from cotton andHibiscus sabdariffa, respectively, when compared to that of the purchased cellulose. In addition, TMA revealed that the average CTE value for the neat ABS and 1 : 1 ratio of cellulose to ABS fabricated in this study was significantly lower than the reported CTE (ca. 73.8 μm/m°C).