The goal of this study is to assess the fresh and hardened properties of self-compacting concrete (SCC) prepared using locally available materials. This research includes also the impact of polypropylene (PP), steel and hybrid fibers on the same properties. In addition, the mechanical properties of SCC specimens (with and without fibers) at high temperatures, including as compressive, tensile, and flexural strengths, will be determined. Four different SCC mixtures (with and without fibers) are prepared, tested, and assessed in order to attain these goals. The specimens were heated to various temperatures (200, 400, 600, and 800) at a rate of 5 degrees Celsius per minute for each test. The temperature was remained constant at the target temperature for one hour before cooling to ensure a consistent temperature throughout the specimen. According to the test results, all of the mixes have good consistency and workability in terms of filling and passing ability. In addition, the inclusion of fibers lowered the workability of SCC slightly. Also, the compressive, tensile, and flexural strengths improved with increasing temperature up to 200 °C and dropped at temperatures over 200 °C, according to these findings. Within the SCC, the PP fibers lowered and removed the risk of spalling. Concrete mixtures containing steel fibers and hybrid fibers have the finest mechanical characteristics and spalling resistance as temperature rises. Weight losses were lower in SCC mixtures with PP and steel fibers than in those without PP and steel fibers. As the temperature rose, all SCC mixes lost mass and UPV decreased until the samples spalled (as in plain SCC and SCC with steel fibers) or were questionable (as in SCC with PP and SCC with hybrid fibers). Doi: 10.28991/cej-2021-03091779 Full Text: PDF
30 September 2022 in Innovative Infrastructure Solutions
The most common effluent created by the oil industry is oily wastewater. This produced water (PW) corrodes the steel piles in the infrastructure of bridges, which shortens their service life. It is important to remove organic content in PW to prevent this outcome. Samples from the Ahdab oil field were used in this study. Two catalysts were selected: zinc oxide (ZnO) and titanium dioxide (TiO2) with photo presence as an energy source. The results were organic elimination of 96.4% and 93.4% using ZnO and TiO2, respectively. The experimental conditions were pH = 3 and an irradiation time of 120 min. Due to the ability of ZnO to adsorb high amounts of organic content from PW, there was an increased elimination of organic content. Hence, the maintenance of steel piles durability is a good alternative to approach the goals of this study. The results of the study demonstrated that the organic adsorption on a catalyst agent reinforced in nonappearance of radiation photo is insignificant.
In this work, the properties of self-compacting concrete (SCC) and SCC containing 0.5 and 1% glass fibers (with lengths of 6 and 13 mm) were experimentally investigated, as well as their performance at high temperatures. With a heating rate of 5 °C/min, high-temperature experiments were conducted at 200, 400, 600, and 800 °C to examine mass loss, spalling, and the remaining mechanical properties of SCC with and without glass fibers. According to the results of the flowability and passing ability tests, adding glass fibers does not affect how workable and self-compacting SCCs were. These findings also demonstrated that the mechanical properties of samples with and without glass fibers rose up to 200 °C but then decreased at 400 °C, whereas the mixture containing 0.5% glass fibers of a length of 13 mm displayed better mechanical properties. Both SCC samples with and without glass fibers remained intact at 200 °C. Some SCC samples displayed some corner and edge spalling when the temperature reached about 400 °C. Above 400 °C, a significant number of microcracks started to form. SCC samples quickly spalled and were completely destroyed between 600 and 800 °C. According to the results, glass fibers cannot stop SCC from spalling during a fire. Between 200 and 400 °C, there was no discernible mass loss. At 600 °C, mass loss starts to accelerate quickly, and it increased more than ten times beyond 200 °C. The ultrasonic pulse velocity (UPV) of SCC samples with glass fibers increased between room temperature and 200 °C, and the mixture containing 0.5% glass fibers of a length of 13 mm showed a somewhat higher UPV than other SCC mixtures until it started to decline at about 400 °C.
The technical and economic effects of the two methods of retrofitting with buckling restrain bracing and using concrete shear wall were investigated. The results of this study showed that using reinforcement, the amount of target displacement in the models was significantly reduced and it was observed that the concrete shear wall had a greater impact on the structure in this regard. The reinforcement methods used in this research have a significant impact on improving the technical performance of structures, which has been more in the strengthening method with concrete shear wall. Also, the evaluations showed that despite the fact that the shear wall of reinforced concrete has a better effect on the performance of the structure from a technical point of view, but in terms of weight, it can be seen that using a buckling brace can be more economical.
The aim of this research was to determine the minimal requirements for shear reinforcement for reactive powder concrete (RPC) rectangular cross-sectional beams with a compressive strength of 157 MPa and a steel fiber volume content of 2.0% that remained constant for all the tested beams. Additionally, the recommendations of KCI-2012 and AFGC-2013 for the design of RPC beams as well as the shear design requirements of ACI 314-2014 when applied to RPC beams were studied. Utilizing a three-dimensional finite element program, a computational model was designed for forecasting the deformations and shear strength of the examined RPC beams. Both the shear-span-to-depth relationship (a/d) and the minimal reinforcement web ratio, represented by the distance between stirrups and the diameter of the stirrup bars, are the key study parameters in this regard. According to this study’s experimental findings, increasing the given reinforcement of the web ratio has little influence on both the ultimate shear strength as well as the diagonal cracking strength of the beams. Additionally, the findings demonstrated that the ACI 318-2014 maximum stirrup spacing requirement of 0.5 d can safely be extended to 0.75 d for beams that are relatively short. Compared to what ACI 318-2014 mandates, the suggestions of AFGC-2013 and KCI-2012 are more cautious and safe. According to the AFGC-2013 criteria, the mean proportion of Vfb to projected Vu,AFGC is roughly 58.3%, whereas the mean proportion of vs. and Vc is just 41.7%. The deformation response and ultimate shear strength of the examined RPC beams were well predicted by the designed model using finite elements when metal fibers were taken into account.