In this paper, we experimentally investigated the integrated processing of high-iron Kazakh bauxites by reducing smelting of ore–coke–lime briquettes to produce an Fe-Al-Si metallic alloy, which is of potential interest for steel deoxidation, together with calcium-aluminate slag, which is of potential interest for alumina extraction. Briquettes containing bauxite, metallurgical coke (10–20 wt.%), and freshly calcined lime (10 wt.%, constant) were melted in a muffle furnace at a temperature of 1200–1450 °C. Complete separation of metal and slag was achieved at 1400–1450 °C, whereas at 1200–1350 °C, separation remained incomplete. Changing the coke/bauxite mass ratio in the charge from 0.125 to 0.286 increased the total content of metallic Si, Al and Fe in the recovered metallic product from 77.1 to 98.66 wt.%, according to X-ray fluorescence (XRF) analysis after two-stage magnetic separation; the metallic product obtained with a coke/bauxite ratio of 0.286 in the charge contained 72.8% Fe, 23% Al and 2.86% Si (with minor impurities of Ti, Mn and Cr), while the associated slag was represented mainly by CaO (59.5%) and Al2O3 (34.0%). These slag characteristics indicate its potential suitability for alumina extraction or as a filler for structural concrete. The proposed route represents a potentially low-waste alternative for processing high-iron bauxites that are poorly suited to the classical Bayer process, avoiding the direct formation of red mud and supporting Kazakhstan’s transition toward closed-loop bauxite processing.
6 October 2025 in Engineering, Technology & Applied Science Research
This study investigated the use of coke for the recovery of minerals included in the composition of ferruginous sands of the alumina production from bauxites of Kazakhstan. The granulometric and mineralogical analyses showed that that fine ferruginous sands were enriched with iron oxides (up to 67.8% Fe₂O₃), while the coarse fractions possessed higher alumina concentrations, primarily in gibbsite and kaolinite. The reduction experiments were conducted using ore-coke-lime briquettes, which were prepared from ferruginous sands (0.40 - 0.63 mm fraction), metallurgical coke, lime, and bentonite. The testing of smelting from 1200 - 1450 °C, demonstrated that the metallic iron was completely separated from slag at 1400–1450 °C, obtaining a metallic phase with 92.62% Fe. The coke content influenced the reduction efficiency, with results obtained at up to 20% coke. The product of the metallic phase was analyzed by X-Ray Fluorescence (XRF), confirming the high purity of the metallic product, while the slag phase, rich in Al₂O₃, SiO₂, and CaO, was successfully tested as a filler in concrete production. The analysis of the chemical composition of the resulting slag revealed the possibility of its use as a filler in the production of construction concrete.