This study investigates the depth-dependent crack-healing behavior of microbially induced calcium carbonate precipitation (MICP) using a novel transparent acrylic mold that enables non-destructive, real-time observation of precipitation across the crack depth in a controlled visualization model. Mortar specimens incorporating fly ash (30%), silica fume (10%), and crystalline admixture (2%) were evaluated to assess the influence of binder composition on MICP-related calcium accumulation. The crack healing process was conducted and monitored over a period of 28 days, and later, calcium accumulation was quantified using an EDTA titration method. The results show that MICP exhibits non-uniform, depth-dependent behavior, with precipitation initiating near the crack opening and progressing toward deeper regions over time. Limited oxygen availability and sustained moisture in deeper zones appear to restrict in situ MICP precipitation, suggesting a possible transition from reaction-controlled to transport-limited conditions. Among the mixtures, fly ash mortar demonstrated the highest calcium accumulation, while silica fume mortar showed the lowest. The findings show an important role of calcium availability and environmental conditions on the performance of MICP and the proposed technique, and they also provide more detail in observing the behavior of MICP across the crack depth.
This study investigated the use of calcined seashell ash (CSA) as a Ca-rich modifier to enhance the mechanical performance and CO2 mineralization of high-calcium fly ash-based alkali-activated mortar. CSA was incorporated at 0–20% replacement levels, while liquid-to-binder (L/B) ratios of 0.35, 0.40, and 0.45 were investigated. Fresh and mechanical properties were evaluated through spread flow, initial setting time, compressive strength, and flexural strength tests. Mineral carbonation was assessed using accelerated carbonation depth, X-ray diffraction (XRD), and thermogravimetric/derivative thermogravimetric (TG/DTG) analyses. Increasing CSA content generally reduced flowability and shortened initial setting time, while 15% CSA produced the highest mean 28-day mechanical strengths. At this level, the 28-day compressive strength increased by 11.5–38.8%, depending on the L/B ratio, while the 28-day flexural strength increased by approximately 102–107% relative to the corresponding mixtures without CSA. Carbonation behavior was strongly influenced by the L/B ratio. At 20% CSA replacement, the carbonation-depth enhancement factor (CEFx) relative to the corresponding mixture without CSA increased from only 1.2% at L/B = 0.35 to 13.2% and 16.6% at L/B = 0.40 and 0.45, respectively. XRD revealed substantially increased calcite-related diffraction features following accelerated carbonation, particularly in the CSA-containing mixtures, while TG/DTG showed a stronger carbonation-associated thermal response for the mixture containing 20% CSA at L/B = 0.45 than for the corresponding mixture without CSA. Together with the carbonation-depth results, these complementary observations consistently indicate that CSA enhanced CO2 mineralization through increased carbonate formation under accelerated CO2 exposure. However, the absolute amount of chemically bound CO2 was not directly quantified in the present study. Overall, CSA can function as both a partial fly ash replacement and a Ca-rich modifier, with its mineral carbonation response governed by the balance between the availability of Ca-bearing phases and CO2 accessibility within the hardened matrix.
Continuous carbon fiber composites have high strength-to-weight ratios, excellent corrosion resistance, and impressive durability. In civil engineering, continuous carbon fiber reinforcement is commonly employed in carbon fiber-reinforced polymer (CFRP) systems, whereas its direct incorporation into low-carbon alkali-activated binder (AAB) matrices remains relatively unexplored. This study presents a preliminary investigation into the fabrication of continuous carbon fiber-reinforced alkali-activated binder (CFR-AAB) composites using a hand lay-up technique. To facilitate fiber impregnation and laminate fabrication, the AAB matrix was first optimized by varying the liquid-to-binder ratio, sodium silicate-to-sodium hydroxide ratio, and sodium hydroxide concentration to balance flowability, setting time, and compressive strength. Using the optimized AAB matrix, which satisfied the adopted flowability and initial setting-time requirements for hand lay-up fabrication while achieving a compressive strength of 48.6 MPa, CFR-AAB laminates containing 12, 24, and 36 carbon fiber plies with symmetric stacking sequences were fabricated and mechanically evaluated. The incorporation of continuous carbon fiber had only a limited influence on compressive strength, with all CFR-AAB configurations achieving values above 46 MPa. In contrast, flexural strength increased substantially from 4.21 MPa for the plain AAB matrix to 70–85 MPa for the CFR-AAB composites, representing more than a sixteen-fold improvement. Failure observations showed that the flexural response was governed mainly by interlaminar delamination and shear-related damage rather than fiber rupture, highlighting the importance of fiber–matrix and interlaminar interactions in controlling composite performance. Overall, this study demonstrates the technical feasibility of manufacturing CFR-AAB composites using a simple hand lay-up process and establishes a foundation for lightweight, low-carbon structural composites. Future research should focus on improving fiber–matrix interfacial bonding and impregnation quality, optimizing laminate configurations, and evaluating the long-term mechanical and durability performance of the composites.