Biodegradable poly(lactide)/poly(butylene adipate-co-terephthalate) (PLA/PBAT) blends were prepared by reactive blending in the presence of chain-extenders. Two chain-extenders with multi-epoxy groups were studied. The effect of chain-extenders on the morphology, mechanical properties, thermal behavior, and hydrolytic degradation of the blends was investigated. The compatibility between the PLA and PBAT was significantly improved by in situ formation of PLA-co-PBAT copolymers in the presence of the chain-extenders, results in an enhanced ductility of the blends, e.g., the elongation at break was increased to 500% without any decrease in the tensile strength. The differential scanning calorimeter (DSC) results reveal that cold crystallization of PLA was enhanced due to heterogeneous nucleation effect of the in situ compatibilized PBAT domains. As known before, PLA is sensitive to hydrolysis and in the presence of PBAT and the chain-extenders, the hydrolytic degradation of the blend was evident. A three-stage hydrolysis mechanism for the system is proposed based on a study of weight loss and molecular weight reduction of the samples and the pH variation of the degradation medium.
In this work, PVA nanocomposite films containing cellulose nanocrystals (CNC) and different amounts of lignin nanoparticles (LNP), prepared via a facile solvent cast method, were crosslinked by adding glutaraldehyde (GD). The primary objective was to investigate the effects of crosslinker and bio-based nanofillers loading on thermal, mechanical, antioxidant and water barrier behaviour of PVA nanocomposite films for active food packaging. Thermogravimetric analysis showed improved thermal stability, due to the strong interactions between LNP, CNC and PVA in the presence of GD, while Wide-angle X-ray diffraction results confirmed a negative effect on crystallinity, due to enhanced crosslinking interactions between the nanofillers and PVA matrix. Meanwhile, the tensile strength of PVA-2CNC-1LNP increased from 26 for neat PVA to 35.4 MPa, without sacrificing the ductility, which could be explained by a sacrificial hydrogen bond reinforcing mechanism induced by spherical-like LNP. UV irradiation shielding effect was detected for LNP containing PVA films, also migrating ingredients from PVA nanocomposite films induced radical scavenging activity (RSA) in the produced films in presence of LNP. Furthermore, PVA-CNC-LNP films crosslinked by GD showed marked barrier ability to water vapour.
17 June 2020 in ACS Sustainable Chemistry & Engineering