In the present work, we have investigated concentration and temperature dependences of electrical conductivity of graphite nanoplatelets/epoxy resin composites. The content of nanocarbon filler is varied from 0.01 to 0.05 volume fraction. Before incorporation into the epoxy resin, the graphite nanoplatelets were subjected to ultraviolet ozone treatment at 20-min ultraviolet exposure. The electric resistance of the samples was measured by two- or four-probe method and teraohmmeter E6-13. Several characterization techniques were employed to identify the mechanisms behind the improvements in the electrical properties, including SEM and FTIR spectrum analysis. It is established that the changes of the relative intensities of the bands in FTIR spectra indicate the destruction of the carboxyl group –COOH and group –OH. Electrical conductivity of composites has percolation character and graphite nanoplatelets (ultraviolet ozone treatment for 20 min) addition which leads to a decrease of percolation threshold 0.005 volume fraction and increase values of electrical conductivity (by 2–3 orders of magnitude) above the percolation threshold in comparison with composite materials—graphite nanoplatelets/epoxy resin. The changes of the value and behavior of temperature dependences of the electrical resistivity of epoxy composites with ultraviolet/ozone-treated graphite nanoparticles have been analyzed within the model of effective electrical conductivity. The model takes into account the own electrical conductivity of the filler and the value of contact electric resistance between the filler particles of the formation of continuous conductive pathways.
29 January 2016 in Materialwissenschaft und Werkstofftechnik
Graphite nanoplatelets (GNPs)—the segregated ultra-high molecular weight polyethylene (UHMWPE)-based composites with hybrid filler—decorated with Fe3O4 were developed. Using X-ray diffraction and scanning electron microscopy, it was shown that the decorated component has the shape of separate granules, or their clusters were distributed evenly over the GNPs surface. The individual Fe3O4 nanoparticles are predominantly rounded, with diameters of approximately 20–60 nm. The use of GNPs/Fe3O4 as a filler leads to significant decreases in the percolation limit φc, 0.97 vol% vs. 0.56 vol% for GNPs/UHMWPE- and (GNPs/Fe3O4)/UHMWPE segregated composite material (SCM), respectively. Modification of the GNP surface with Fe3O4 leads to an essential improvement in the electromagnetic interference shielding due to enhanced microwave absorption in the 26–37 GHz frequency range in its turn by abundant surface functional groups and lattice defects of GNPs/Fe3O4 nanoparticles.