Ice accumulation on outdoor surfaces tends to cause a series of serious accidents in extreme climates. In recent years, superhydrophobic coatings have garnered significant interest in the passive anti-icing field owing to their exceptional ability to repel water. However, these superhydrophobic coatings displayed inadequate anti-icing properties in conditions of low temperature and high humidity, as well as poor corrosion resistance after prolonged immersion. Herein, we prepared a series of modified graphene micropillar array superhydrophobic coatings that have various micropillar widths based on simple physical embossing and spraying techniques. These coatings combined the graphene nanosheets modified by perfluorodecyl triethoxysilane (AC-FAS) and the fluorocarbon varnish coating with a micropillar array structure to gain great superhydrophobicity and anti-icing properties. Among these, the average freezing delay time of the Q200G coating increased over 500 times relative to the unmodified Al surface (about 10 s), and its average deicing shear force was as low as 0.1 N. Meanwhile, the corrosion resistance increased steadily as the micropillar width decreased, based on the electrochemical impedance spectroscopy test results. More importantly, such facile fabrication methods and multi-functionality make superhydrophobic coatings hold great application prospects.
The effects of stacking configuration on the environmental durability of carbon fiber-reinforced polymer (CFRP) laminates were investigated under hygrothermal and salt spray aging. Unidirectional [0]n and cross-ply [0/90]n laminates were aged for up to 42 d, and their moisture absorption, chemical structure, dynamic mechanical behavior, flexural properties, and fracture characteristics were evaluated. Hygrothermal exposure produced higher moisture uptake and diffusion rates than salt spray, while the Langmuir model described the absorption behavior more accurately than the Fick model. After 42 d, the glass transition temperatures of the [0]n and [0/90]n laminates decreased by 23.8% and 23.7% under hygrothermal aging compared with 9.0% and 6.9% under salt spray. The corresponding flexural-strength losses were 16.1% and 18.6% versus 9.6% and 10.7%. Although the [0/90]n laminate exhibited slightly lower moisture uptake, it suffered greater strength degradation because transverse cracking in the 90° plies promoted interfacial debonding and delamination. These results show that the environment governs degradation intensity, whereas stacking configuration controls damage propagation and flexural failure.