Aybüke uslu tekce

Dr. Aybüke uslu tekce

orcid

Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
12 July 2022 in Lasers in Medical Science
Verified
Journal Article
Closed access
PDF file
ATAybüke uslu tekce
Aybüke uslu tekce
AYA. Ruya Yazici
A. Ruya Yazici

29 September 2022 in Journal of Esthetic and Restorative Dentistry
Verified
Journal Article
Closed access
MDMeltem Nermin Dursun
Meltem Nermin Dursun
EEEsra Ergin
Esra Ergin
ATAybüke uslu tekce
Aybüke uslu tekce
SEVIL GURGANSEVIL GURGAN
SEVIL GURGAN

26 October 2021 in Clinical and Experimental Health Sciences
Verified
Journal Article
Closed access
ATAybüke uslu tekce
Aybüke uslu tekce
CACansu Atalay
Cansu Atalay
MDMeltem Nermin Dursun
Meltem Nermin Dursun
AEA. Atila Ertan
A. Atila Ertan
AYA. Rüya Yazici
A. Rüya Yazici
Objective: evaluate the influence of single- or double-layer application of a universal adhesive on the bond strength to different tooth substrates. Methods: To Seventy-two extracted sound human teeth were used for the study. The teeth were divided into three groups according to tooth substrates; enamel, coronal and radicular dentin (n=24). The roots of the teeth were separated from the crowns and then abraded to obtain flat surfaces. The specimens were randomly allocated into 2 groups in accordance with application layers of universal adhesive (n=12). The universal adhesive, Adhese Universal was applied in self-etch mode as single- or double-layer (without light-curing of the first layer) to different substrates. Following the adhesive application, enamel, coronal- and radicular dentin substrates were restored with a resin composite (Tetric N-Ceram). The specimens were subjected to shear bond strength (SBS) test after storage in distilled water (37℃,24 h). Representative fractured and interface samples from each group were examined by a scanning electron microscope. The data were analyzed using two-way ANOVA(α = 0.05). Results: There was no statistically difference in SBS values between single- and double-layer applications of the tested universal adhesive on different dental substrates (p>0.05). Whilst no difference was occurred between the different dental substrates in the single-layer application (p>0.05), double-layer application on coronal dentin presented significantly higher bond strength than enamel (p

31 December 2021 in Selcuk Dental Journal
Verified
Journal Article
Closed access
CACansu Atalay
Cansu Atalay
ATAybüke uslu tekce
Aybüke uslu tekce
EMEce Meral
Ece Meral
AYAyşe YAZICI
Ayşe YAZICI
AEA. Atila Ertan
A. Atila Ertan
Amaç: Bu in vitro çalışmanın amacı, tükürük kontaminasyonu/dekontaminasyon yöntemlerinin polimerize olmuş bir üniversal adezivin dentine bağlanma dayanımı üzerindeki etkisini değerlendirmektir. Gereç ve Yöntem: Çalışma için 70 adet çekilmiş insan azı dişi kullanıldı. Dişler meziodistal olarak boylamasına kesildikten sonra standart bir dentin yüzeyi elde etmek için aşındırıldı. Dişlere üniversal adeziv (Adhese, Ivoclar/Vivadent) uygulanıp polimerize edildikten sonra tükürük kontaminasyon yöntemlerine (n=14) göre rastgele beş gruba ayrıldı: Grup I-Kontaminasyon yok (kontrol); Grup II: Adeziv / Tükürük /Yıkama; Grup III: Adeziv /Tükürük /Kurutma /Adeziv; Grup IV: Adeziv /Tükürük /Yıkama /Kurutma; Grup V: Adeziv /Tükürük /Yıkama /Kurutma /Adeziv. Yüzeylere kompozit silindirler (Tetric N-Ceram) uygulandı. Örnekler distile suda 24 saat bekletildkten sonra kesme bağlanma dayanımları üniversal test cihazı kullanılarak ölçüldü. Veriler tek yönlü ANOVA ve Tukey çoklu karşılaştırma testi kullanılarak analiz edildi (p 0.05). Grup IV ve V, test edilen diğer gruplara göre istatistiksel olarak daha düşük bağlanma dayanımı değerleri gösterdi (p 0.05). Sonuç: Havayla kurutma ile dekontaminasyon, kontrol grubuna benzer bağlanma dayanımı değerleri ile sonuçlanmıştır. Suyla durulama/havayla kurutma ile dekontaminasyon düşük bağlanma dayanımı değerlerine sebep olmuştur. Dekontaminasyon yönteminden bağımsız olarak, adezivin tekrar uygulanması bağlanma dayanımını etkilememiştir.