Matouš Uhlík

Mr. Matouš Uhlík

orcid

Research Focus & Metrics

Academic Career Length

1Year (2026-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
14 September 2026 in Materials Science and Engineering: A
Verified
Journal Article
Open access
VRVishnu Ramasamy
Vishnu Ramasamy
BLBrett Edward Ley
Brett Edward Ley
JDJan Dzugan
Jan Dzugan
MUMatouš Uhlík
Matouš Uhlík
JCJennifer L.W. Carter
Jennifer L.W. Carter
JLJohn Lewandowski
John Lewandowski

29 September 2026 in Results in Engineering
Verified
Journal Article
Open access
SPSlavomír Parma
Slavomír Parma
TVTereza Vaňková
Tereza Vaňková
RMRené Marek
René Marek
HFHeidi P. Feigenbaum
Heidi P. Feigenbaum
DGDušan Gabriel
Dušan Gabriel
YDYannis F. Dafalias
Yannis F. Dafalias

16 November 2026 in Materials
Verified
Journal Article
Open access
PDF file
MPMichal Povolný
Michal Povolný
MUMatouš Uhlík
Matouš Uhlík
JFJakub Fousek
Jakub Fousek
JMJan Matoušek
Jan Matoušek
JSJosef Sklenička
Josef Sklenička
Jan DzuganJan Dzugan
Jan Dzugan
Surface preparation represents a critical step in high-cycle fatigue (HCF) testing of miniature specimens, where even small variations in surface integrity may significantly affect crack initiation and increase experimental scatter. This study presents a statistical optimisation of the longitudinal polishing process for miniature 22CrMoNiWV8-8 (EN 1.6945) steel fatigue specimens using Response Surface Methodology combined with Analysis of Covariance (RSM-ANCOVA). A Design of Experiments consisting of 60 polishing trials was performed to investigate the effects of abrasive belt speed, feed rate, contact setting, and abrasive belt type, while the initial surface roughness was incorporated as a covariate. The analysis confirmed that the initial roughness significantly influenced the polishing response and therefore had to be considered during process optimisation. Among the investigated factors, abrasive belt type exhibited the strongest effect on the final surface quality. The medium abrasive belt achieved the highest adjusted mean roughness reduction (EMM = 0.282 µm) and the lowest variability of the final surface roughness and significantly outperformed the coarse belt (p < 0.001), while no statistically significant difference was observed between the medium and fine belts. Belt-specific RSM–ANCOVA models were used to describe differences in the response to polishing parameters. The proposed methodology supports the control of surface roughness in miniature specimens intended for HCF testing. Its effects on fatigue strength, fatigue life and fatigue-result variability require separate experimental verification.

24 June 2026 in SSRN Electronic Journal
Verified
Preprint
Open access
VRVishnu Ramasamy
Vishnu Ramasamy
BLBrett Edward Ley
Brett Edward Ley
Jan DzuganJan Dzugan
Jan Dzugan
MUMatouš Uhlík
Matouš Uhlík
JCJennifer Carter
Jennifer Carter
JLJohn Lewandowski
John Lewandowski
This study investigates elastic anisotropy in thick-walled 316LSi stainless steel deposits fabricated by Wire Arc Additive Manufacturing (WAAM). Four deposition conditions were evaluated by varying heat input (10 and 15 kJ/in.) and interpass temperature (121 and 399 °C), while maintaining a consistent alternating parallel toolpath strategy with 45% bead overlap. Optical metallography revealed that this tool path promoted cyclic partial remelting and produced a distinct periodic, wavy columnar grain morphology. Electron Backscatter Diffraction (EBSD) indicated corresponding crystallographic texture tendencies, with ⟨100⟩ alignment along the deposition direction (X-axis) and ⟨111⟩ alignment along the transverse direction (Y-axis). Since ⟨111⟩ is the stiffest and ⟨100⟩ is the most compliant crystallographic direction in FCC 316L/316LSi, these texture tendencies provide a mechanistic basis for the observed macroscopic elastic anisotropy. Room-temperature tensile testing and resonant frequency and damping analysis (RFDA) from 23 °C to 400 °C confirmed a consistent orientation-dependent modulus hierarchy of EY > EZ > EX. The lowest Young’s modulus values were consistently measured along the deposition direction (X-axis: 146 to 150 GPa), while the highest values were observed along the transverse direction (Y-axis: 187 to 197 GPa). Overall, elastic anisotropy was governed primarily by the toolpath-induced microstructure and crystallographic texture, rather than by variations in heat input or interpass temperature within the processing window studied. The modulus hierarchy also persisted up to 400 °C, indicating stable anisotropic elastic behavior under the tested thermal exposure conditions.