Irradiation by ionizing radiation is a specific type of controllable modification of the physical and chemical properties of a wide range of polymers, which is, in comparison to traditional chemical methods, rapid, non-polluting, simple, and relatively cheap. In the presented paper, the influence of high-energy ionizing radiation on the basic mechanical properties of the melamine resin, phenol-formaldehyde resin, and nitrile rubber blend has been studied for the first time. The mechanical properties of irradiated samples were compared to those of non-irradiated materials. It was found that radiation doses up to 150 kGy improved the mechanical properties of the tested materials in terms of a significant increase in stress at break, tensile strength, and tensile modulus at 40% strain, while decreasing the value of strain at break. At radiation doses above 150 kGy, the irradiated polymer blend is already degrading, and its tensile characteristics significantly deteriorate. An radiation dose of 150 kGy thus appears to be optimal from the viewpoint of achieving significant improvement, and the radiation treatment of the given polymeric blend by a beam of accelerated electrons is a very promising alternative to the traditional chemical mode of treatment which impacts the environment.
1 February 2020 in IOP Conference Series: Materials Science and Engineering
This paper is focused on the preparation of polymer blends with addition of alternative filler from glass industry in various granularity (>40 µm, 40–32 µm, 32–25 µm, 25–0 µm). The polymer matrix (PMX3) consists of melamine resin, phenolic resin and nitrile rubber. This polymer matrix composition is commonly applied in friction composite systems in automotive industry. The surface activity of various filler fractions was studied. The rheological properties, such as minimum torque, maximum torque, optimum vulcanization time and scorch time of prepared friction polymer matrix were tested, using the PRPA 2000 rheometer. Mooney viscosity of new prepared polymer matrix was studied with help of Mooney Viscosimetr 91.03 Gottert testing machine.