In this study, 2198 Al-Li alloy, a low density and high-performance material for aerospace equipment, was welded using ultrahigh-frequency pulse alternating current with cold metal transfer (UHF-ACCMT). Influence of different ultrahigh-frequency on the formation, porosity, microstructure, microhardness and tensile strength of the welded joints were investigated. The results showed that the coupled ultrahigh-frequency current generated electromagnetic force to stir the liquid metal of molten pool. The weld formation became much better with metallic luster and uniform ripples at frequency of 60 kHz and 70 kHz. The porosity was the minimum at frequency of 60 kHz. Furthermore, the molten pool was scoured and stirred by the electromagnetic force which provided the thermal and dynamic conditions for nucleation and grain refinement, the width of fine equiaxed grain zone became larger, and the number of equiaxed non-dendrite grains increased. With the grain refining and crystallize transition, the average microhardness and tensile strength of the joints at frequency of 60 kHz reached up the highest value, 116 HV0.1 and 338 MPa, respectively. The fracture of the welded joints presented the characteristics of quasi-cleavage fracture.
16 October 2018 in High Temperature Materials and Processes
6082-T6 aluminum alloy plate with thickness of 42mm was butt welded by friction stir welding (FSW) from two sides. The microstructures of the joints exhibited different grain sizes because of unequal frictional heating and plastic flow during FSW process. The transition from the heat affected zone (HAZ) to the nugget zone (NZ) in thermos-mechanical affected zone of advancing side (AS-TMAZ) was more sudden than thermos-mechanical affected zone of retreating side (RS-TMAZ). Kissing bond (KB) defect throughout the entire FSW joint was displayed both at the grain boundary and in the interior of the grain with semi-continuous bands. KB had no direct effect on tensile properties. Vickers hardness of the FSW joint was lower than the BM because its high heat input, dissolved and coarsened precipitates and little to the grain size after FSW. Hardness distribution of double-sided welding joint showed X-shaped area softening characteristics, that is to say the lowest hardness was the junction of two welding joint of NZ and the junction of TMAZ and HAZ. The tensile fracture position occurred in the lowest hardness region of the FSW joint, and it did not occur in the KB defect position.
1 January 2021 in High Temperature Materials and Processes
Al–Li alloy has been widely used in the aerospace field owing to its high strength and low density. In this study, alternating current cold metal transfer (AC CMT) along with a high-frequency pulse current technique was used to weld a 2060 Al–Li alloy using an ER5356 wire. The effect of pulse frequency on the arc shape, microstructure, and mechanical properties of the welded joints was examined, and mechanical performance testing was conducted. The results revealed that the arc diameter, arc length, and arc volume showed a trend of increasing first and then decreasing with an increase in the pulse frequency and reached their peak values when the pulse frequency was 50 kHz. Coupling the welding process with a high-frequency pulse resulted in grain refinement, which was attributed to the stirring action of the arc force. Both the porosity levels and grain size decreased with increasing frequency. When the pulse frequency was 70 kHz, the porosity level was the lowest, and the grain size was refined to 24.1 μm. The tensile strength of the welded joints also increased with the pulse frequency, and a maximum tensile strength of 249 MPa was observed at 70 kHz.
Sn–Sb system solders and ENIG/ENEPIG surface finish layers are commonly used in electronic products. To illustrate the thermal reliability evaluation of such solder joints, we studied the interfacial microstructure and shear properties of Sn-4.5Sb-3.5Bi-0.1Ag/ENIG and Sn-4.5Sb-3.5Bi-0.1Ag/ENEPIG solder joints after aging at 150 °C for 250, 500 and 1000 h. The results show that the intermetallic compound of Sn-4.5Sb-3.5Bi-0.1Ag/ENIG interface was more continuous and uniform compared with that of Sn-4.5Sb-3.5Bi-0.1Ag/ENEPIG interface after reflow. The thickness of the interfacial intermetallic compounds of the former was significantly thinner than that of the latter before and after aging. With extension of aging time, the former interface was stable, while obvious voids appeared at the interface of the latter after 500 h aging and significant fracture occurred after 1000 h aging. The shear tests proved that shear strength of solder joints decreased with increasing aging time. For the Sn-4.5Sb-3.5Bi-0.1Ag/ENEPIG joint after 1000 h aging, the fracture mode is ductile-brittle mixed type, which means fracture could occur at the solder matrix or the solder/IMC interface. For other samples of these two types of joints, ductile fracture occurred inside of the solder. The Sn-4.5Sb-3.5Bi-0.1Ag/ENIG solder joint was thermally more reliable than Sn-4.5Sb-3.5Bi-0.1Ag/ENEPIG.