Lithium phenyl (2,4,6-trimethylbenzoyl) phosphinate (LAP) is a free radical photo-initiator used to initiate free radical chain polymerization upon light exposure, and is combined with gelatin methacryloyl (GelMA) to produce a photopolymer used in bioprinting. The free radicals produced under bioprinting conditions are potentially cytotoxic and mutagenic. Since these photo-generated free radicals are highly-reactive but short-lived, toxicity assessments should be conducted with light exposure. In this study, photorheology determined that 10 min exposure to 9.6 mW/cm2 405 nm light from an LED light source fully crosslinked 10 wt % GelMA with >3.4 mmol/L LAP, conditions that were used for subsequent cytotoxicity and mutagenicity assessments. These conditions were cytotoxic to M-1 mouse kidney collecting duct cells, a cell type susceptible to lithium toxicity. Exposure to ≤17 mmol/L (0.5 wt %) LAP without light was not cytotoxic; however, concurrent exposure to ≥3.4 mmol/L LAP and light was cytotoxic. No condition of LAP and/or light exposure evaluated was mutagenic in bacterial reverse mutation assays using S. typhimurium strains TA98, TA100 and E. coli WP2 uvrA. These data indicate that the combination of LAP and free radicals generated from photo-excited LAP is cytotoxic, but mutagenicity was not observed in bacteria under typical bioprinting conditions.
29 October 2007 in Journal of Biomedical Materials Research Part B: Applied Biomaterials
Potential connections between release profiles and solvent evaporation rates alongside polymer chemistry were elucidated for the release of tetracycline hydrochloride from two different poly (d, l-lactide-co-glycolide) (PLGA) film matrices containing high drug fractions (50%, 30%, and 15%), and prepared at two distinct solvent evaporation rates. At highest tetracycline concentrations (50%), (i) the early release rates were ≤0.5 μg/min in all cases; (ii) release was linear from systems fabricated with lower lactic content and slower solvent evaporation rate and bimodal from systems fabricated with higher lactic content and faster evaporation rate; (iii) surface fractions covered by the drug were similar at both evaporation rates for 85:15 PLGA but very different for 50:50 PLGA, leading to unexpectedly reduced early release from 50:50 PLGA than from 85:15 PLGA when both the matrices were fabricated using a slower evaporation rate. These features remained unaffected in case of low drug concentration. Results suggested that during the formation of the drug-polymer microstructure, the combined effect of polymer chemistry and solvent evaporation rate sets apart the surface characteristics and the initial release profiles of systems containing high drug fraction, and an appropriate combination of these parameters may be utilized to control the early stage of drug release.
7 April 2023 in Materials Performance and Characterization
Despite the proliferation of over-the-counter (OTC) personal lubricants (PLs) in the last two decades, to date, no known positive control has been identified to assess the compatibility of these PLs with polyurethane (PU) condoms. In the absence of suitable positive controls, PU condom compatibility with OTC PLs is assessed using a method built for testing compatibility of latex condoms with PLs. Herein, we attempt to identify a safe-to-handle positive control(s) for determining PU condom-lubricant compatibility. At room temperature (RmT), swelling of and induced stress in PU condom sample coupons were studied at various strain rates after discrete applications of a few ingredients common in commercial PLs. Additionally, stress reduction at a constant stretch was measured at 37°C. At low strain rates, changes in the induced stress and stress-to-strain ratio were detectable because of ingredients, e.g., hydroxy-terminated poly(dimethyl siloxane) of viscosity 25 cSt that caused substantial swelling of the condom materials at RmT, indicating prospective positive controls. At 37 °C, the percent stress reduction in PU samples under constant stretch was significant, with a few PL ingredients that did not significantly swell the PU material at RmT. Ingredients that enable significant stress reduction can serve as positive controls in PU condom-lubricant compatibility testing using the tensile method, provided the strain rate is comparable to the rate of condom-lubricant interaction, as evidenced by swelling study. At RmT, absence of swelling and insignificant changes in tensile properties at high strain rates do not guarantee the absence of interactions. Instead of testing mineral oil on latex condoms, manufacturers may now use a PU condom-specific positive control, when testing compatibility of PU condoms with OTC PLs.
17 June 2024 in Materials Performance and Characterization
Over-the-counter (OTC) personal lubricants (PLs) generally have less potent effects on condoms’ mechanical properties than do appropriate positive controls. Therefore, to assess the compatibility of OTC PLs with condoms, a test method must be more sensitive than those employed to capture the effect of a strong positive control. Using various percent compositions of selected common ingredients in commercial PLs, we attempted to differentiate between the sensitivities of different methods for testing lubricant effects on polyurethane (PU) condoms. After discrete applications of each composition, we studied induced stresses and stress-to-strain ratios at various strain rates, and stress reduction at a constant stretch, in PU condom coupons at 37°C. Swelling was studied at room temperature (RmT). Changes in the induced stress and stress-to-strain ratio because of low percent composition of a potent surrogate component were detectable only at low strain rates. A few low percent compositions of potent ingredients – though they induced insignificant changes in the material as detected by tensile testing and did not swell the PU material – noticeably reduced the percent stress at a constant stretch. Slower strain rates in tensile testing were necessary to detect the effects of low potency combinations, whereas stress reduction was the most efficient detector of change at a constant physiologically relevant strain. Absence of swelling and insignificant changes in tensile properties at high strain rates did not guarantee an absence of interactions. Manufacturers now have a more sensitive method for capturing the interactions of PU condoms with OTC PLs, which are generally less potent than appropriate positive controls.